Tubing I.D. and Material for 10mm Connectors
For glassware such as these below (barbed connectors are stated as 10mm), what inner diameter of the tubing should I get (6, 7, 8mm)?
If the material are less elastic than rubber, for example silicone, vinyl or Viton, should I get a slightly bigger size?
What material is good for halogens and acids (nitric acid), and vacuum too, value for money wise, as I prolly won't deal with those often?
Cheers.
![](https://i.ebayimg.com/images/g/55AAAOxyBjBTVLJz/s-l400.jpg)
![](https://i.ebayimg.com/images/g/NpQAAOSw1xhZmufg/s-l400.jpg)
![](https://i.ebayimg.com/images/g/AfIAAOSwu4BVlIzg/s-l400.jpg)
|
|
monolithic
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 436
Registered: 5-3-2018
Member Is Offline
Mood: No Mood
|
|
I use 5/16" (7.9 mm) silicone vacuum hose on "10 mm" hose barbs and it works perfectly. You want to undersize it by 1-2 mm to get a tight fit,
assuming your hose material is reasonably flexible. My silicone tubing has held up to organic solvents (xylene, toluene, ethyl acetate, hexanes, etc.)
and some acid fumes (acetic acid mostly) without issue. I doubt it would hold up very well to nitric acid fumes, however.
[Edited on 9-1-2019 by monolithic]
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 771
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
Quote: Originally posted by monolithic ![](images/xpblue/lastpost.gif) | I use 5/16" (7.9 mm) silicone vacuum hose on "10 mm" hose barbs and it works perfectly. You want to undersize it by 1-2 mm to get a tight fit,
assuming your hose material is reasonably flexible. My silicone tubing has held up to organic solvents (xylene, toluene, ethyl acetate, hexanes, etc.)
and some acid fumes (acetic acid mostly) without issue. I doubt it would hold up very well to nitric acid fumes, however.
[Edited on 9-1-2019 by monolithic] |
Silicone rubber is not considered compatible with Xylene, toluene, and hexane. I used it once as fuel line on a chain saw it became very soft but
cracked at the barbs. Of cause its dependent on time and temperature and the type rubber. Some fuel hoses do have a silicone rubber covering but with
a more compatible inner sleeve.
https://mykin.com/rubber-chemical-resistance-chart-3
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
draculic acid69
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
I've always used clear aquarium tubing for everything and it's been fine but now I'm using that shitty brown rubber tubing for condensers as it's not
so stiff which in condenser lines is a good thing.wouldnt use it for anything other than that though.
|
|
monolithic
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 436
Registered: 5-3-2018
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by wg48temp9 ![](images/xpblue/lastpost.gif) | Quote: Originally posted by monolithic ![](images/xpblue/lastpost.gif) | I use 5/16" (7.9 mm) silicone vacuum hose on "10 mm" hose barbs and it works perfectly. You want to undersize it by 1-2 mm to get a tight fit,
assuming your hose material is reasonably flexible. My silicone tubing has held up to organic solvents (xylene, toluene, ethyl acetate, hexanes, etc.)
and some acid fumes (acetic acid mostly) without issue. I doubt it would hold up very well to nitric acid fumes, however.
[Edited on 9-1-2019 by monolithic] |
Silicone rubber is not considered compatible with Xylene, toluene, and hexane. I used it once as fuel line on a chain saw it became very soft but
cracked at the barbs. Of cause its dependent on time and temperature and the type rubber. Some fuel hoses do have a silicone rubber covering but with
a more compatible inner sleeve.
https://mykin.com/rubber-chemical-resistance-chart-3 |
Yes, it is incompatible with direct exposure but after a few hundred distillations it's still holding up. I chose silicone because it was cheap and
easy to find. There are better options, perhaps at a higher cost.
It's also important to consider wall diameter. My tubing was something like 2.5 or 3.0 mm wall diameter, which lets me pull a good vacuum without the
tube collapsing.
[Edited on 9-1-2019 by monolithic]
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
8-10 mm depending on the material and it's thickness.
I used some silicone for NoX and it showed signs of aging very fast. Plain rubber on my vacuum pump didnt look good either after a few distillations.
I now use Viton for almost everything. As a general rule its easier to bend than Teflon but has the same chemical resistance.
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
artemov
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 181
Registered: 22-8-2018
Member Is Offline
|
|
Thanks guys. 8mm silicone/viton it will be
|
|