Unclogging a glass frit


Ok I've used my sintered glass filter for the first time thinking that it would be great for filtering my freshly boiled plant extract and for the first minute it was,then it slowed down,then it almost stopped.anyway hours later I have a finally filtered solution and a frit full of dirt dust and small particles of plant matter clogging it up.are there any tips to get it clean I've tried hot water which helped and ethanol got the green out now I just need to get the brown out.should I try h2so4,or nitric acid? Don't have thf or peroxide
View user's profile View All Posts By User
markx
National Hazard
****




Posts: 645
Registered: 7-8-2003
Location: Northern kingdom
Member Is Offline

Mood: Very Jolly

[*] posted on 20-8-2019 at 22:23


Piranha solution would make quick work on that problem, but since you do not have peroxide available I would suggest to give nitric a try.
Harsh cleaning products based on sulfonic acid may also work....at least I have had success with them unclogging glass frits that were gummed up with organic plant residue.




Exact science is a figment of imagination.......
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 20-8-2019 at 22:47


Can the 3% h2o2 be used for this
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6250
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 20-8-2019 at 23:01


I think that 3% peroxide is likely to be too low to have any real effect. But no harm in giving it a try. Some local pharmacies sell 6% which is more promising. Either way, be prepared to invest a little time.
Nitric acid is a possibility. That would be my next choice.
Or anything that will break down cellulose. Schweitzer's reagent has been suggested for this before.
You might get success with concentrated oxalic acid or a different reducer. Sodium sulfite is sold to accelerate the decomposition of tree stumps.




View user's profile View All Posts By User
j_sum1
Administrator
Thread Moved
20-8-2019 at 23:01
Chemetix
Hazard to Others
***




Posts: 375
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline

Mood: Wavering between lucidity and madness

[*] posted on 20-8-2019 at 23:13


If you are careful about how slowly you heat it up you can leave it in a bunsen flame and it should burn off anything organic, I do this for chemists who have activated carbon stuck in their filters. I have a kiln that goes to 560C and that usually does it, but when I couldn't be bothered running a kiln for a single item they need quickly, the bunsen trick works.

Welders "pickle " is a 30% solution of HNO3 and 2-5 % HF. If used outside with good skin protections and safely glasses it's safe enough, and it takes just about anything inorganic away. It's fairly benign on glassware but leaving it on slightly etched or corroded glass overnight or hot will start to etch into the glass a small amount.
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 20-8-2019 at 23:52


Won't be trying that welders stuff HF scares the shit out of me.ill get a bottle of the 6% peroxide and give that a try.im not sure it's 100% organic I'm sure a good amount of it is literally dirt and bcoz the lawn is so dry every step I take brings up a cloud of dust and i haven't yet come up with a way to successfully filter this stuff out.im guessing diatomaceous earth would be the way to go.lesson learned.
View user's profile View All Posts By User
nimgoldman
Hazard to Others
***




Posts: 303
Registered: 11-6-2018
Member Is Offline


[*] posted on 1-9-2019 at 21:55


I use hot nitric acid, since it is such a strong oxidizer and attacks even metals (sometimes I filter stuff containing copper and silver).

You can concentrate your peroxide, I believe ~10% might work too. Be careful, since addition of H peroxide to sulfuric acid will heat it up a lot because of the water. Also swirl/stir the Piranha constantly and never add more than say 25% v/v of hydrogen peroxide to prevent explosions.

Also note the glass will heat up a lot, maybe pre-heat it to prevent cracking of the thermal expansion.

I always do this inside a Pyrex dish.