I am in the field of manufacturing plasticizer and chlorinated paraffin since last 20 years.
I am on research of advance technic of chlorinated paraffin.
chlorinated paraffin in General a simple reaction of paraffin with Chlorine, it is used to replace partially Di octyl phthalate and other similar plasticizer in processing of PVC compound, it is just react as filler and the weak point of using chlorinated paraffin is migration on period of time.which depends upon dosage of Chlorinated paraffin and type of carbon chain and stabilizers dosage, any body can suggest for any advance technology that replace 100% Primary plasticizer by chlorinated paraffin without any impact?