Chemical Removal of Copper from Graphite Gouging Rods
Hi all,
Looking for some ideas to remove the copper cladding from graphite gouging rods. Obviously there is mechanical removal which I've found to be messy
and very time consuming. I currently have a few rods soaking in a dilute HCl and H2O2 solution, seems to be working okay. Ferric chloride might work
but will probably also contaminate the graphite making it unfavorable for some uses.
I just want to get some input on methods of removal that wont contaminate or degrade the graphite. This is for a video series, so I want to put
multiple methods out there that I may not have thought of.
Cheers
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Electrolysis?
You would want to rotate the rods though.
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
being copper dilute nitric acid looks obvious.
then there's the microwave assisted carbon and hydrogen peroxide, acetic acid and a pinch of salt method ( )
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
rockyit98
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline
Mood: no mood is a good mood
|
|
i did this before ,best way is Electrolysis in dil. sulfuric acid like 5%. use copper cathode so no waste is generated let it run till all copper is
plated on the wire. it will not degrade the graphite if you used low current (1-2A)
|
|
Heptylene
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 319
Registered: 22-10-2016
Member Is Offline
Mood: No Mood
|
|
1M H2SO4 + some H2O2 should work very well.
CuCl2/HCl should work well too, but might leave some CuCl residue.
Both these methods are used for etching copper on printed circuit boards.
If you have nitric acid on hand, it will work even better.
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Commercial leaching of copper is accomplished with ammonia, ammonium carbonate, and air which is a mixed reaction involving some electrochemisty (and
so, as an electrolyte, you might want to add a pinch of sea salt as Ubya suggests, a smart guy, but he apparently uses his microwave for everything,
so I would trust this reference more https://www.researchgate.net/publication/260310630_Ammonia_l... and also this source, where the entire text is available for free at: https://www.academia.edu/292096/Kinetics_and_Mechanism_of_Co... ).
Unfortunately, the cited provided chemistry is even a little more complex with a mention of a minor secondary reaction, as the O2/Cu reaction
complexed with NH3 is akin to a metal/air battery forming instrumental solvated electrons (as sourced from copper, so it is correct to claim that
copper is catalytic to the oxidation of ammonia to nitrite from air). The latter e-(aq), I would surmise, with O2 may introduce the superoxide
radical, and with H+, the hydrogen atom radical, which can interact with NH3 forming •NH2 radical, further interacting with O2 as follows:
•NH2 + O2 → NH2O2• (aminylperoxyl radical unstable) → NO + H2O
As a reference, see "On the aqueous reactions of the aminyl radical with molecular oxygen and the superoxide anion", Page 24, Table 2.1 at http://www.diva-portal.se/smash/get/diva2:730237/FULLTEXT01.... .
where the NO is a precursor to nitrite, and in particular NH4NO2. The latter has the annoying property of suddenly based on pH, of rapidly releasing
volumes of N2 gas, which will cause leakage and even breakage of sealed reaction vessels (as I have experienced).
Some bottom line, don't tightly seal your reaction vessel (and I would recommend avoiding any skin contact with the solution due to possible toxic
ammonium nitrite presence), because the cited minor secondary reaction (which creates NH4NO2) may have consequences.
[Edited on 2-8-2019 by AJKOER]
|
|