Why is my zinc powder not powder???
I bought zinc powder, but most arent powder, they'er large pieces. Why???
|
|
XeonTheMGPony
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1640
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
Usually it is a granular powder, reason is oxidation, Super fine dusts oxidize super fast.
|
|
TmNhRhMgBrSe
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 112
Registered: 4-7-2019
Member Is Offline
|
|
I tried pressing with spatula to break them but they're reallu hard, not because stick by water. I also tried adding the pieces to acid and hydrogen
formed.
|
|
TmNhRhMgBrSe
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 112
Registered: 4-7-2019
Member Is Offline
|
|
But what's the relationship between powder and oxidation, XeonTheMGPony?
|
|
Pumukli
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 696
Registered: 2-3-2014
Location: EU
Member Is Offline
Mood: No Mood
|
|
Powder = big surface area = fast oxidation.
My zinc powder also contains bigger "chunks" and very fine powder particles. I think the "what you pay for is what you get" applies here. ![:)](./images/smilies/smile.gif)
With a fine sieve these powders could be improved. Unfortunately such sieves are not cheap.
Ball milling may help too, but I'm not sure if there were any particular do-s and dont-s regarding ball milling zinc to fine dust.
|
|
Amos
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline
Mood: No
|
|
Maybe take a fine kitchen seive and separate dust and granules to use for separate projects? It's not the end of the world.
|
|
TmNhRhMgBrSe
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 112
Registered: 4-7-2019
Member Is Offline
|
|
Pumukli, but why there are chunks? Why don't the manufacturer powderise all chunks before selling?
[Edited on 19-7-24 by CELamCheng]
[Edited on 19-7-24 by CELamCheng]
|
|
TmNhRhMgBrSe
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 112
Registered: 4-7-2019
Member Is Offline
|
|
I tried used a pliers to press the chunks. They break. Why? Shouldn't they become thinner pieces?
|
|
stygian
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 242
Registered: 19-9-2004
Member Is Offline
Mood: No Mood
|
|
"is zinc malleable" - "Zinc is a bluish-white metal with a shiny surface. It is neither ductile nor malleable at room temperature."
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3027
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
As stated before: Because you didn't pay them to do so.
|
|
RedDwarf
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 166
Registered: 16-2-2019
Location: UK (North West)
Member Is Offline
Mood: Variable
|
|
What are you trying/planning to do with the zinc? For some uses you really don't want powder and turnings or chunks are much better.
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3027
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
I did some organic reductions and it was a pain to keep it cool with the powder I had, but chunks I would imaging would also be a pain as they are
harder to stir.
For reductions I would go for the chunky stuff after sieving, for pyrotechnics I would go for the quality powdered stuff
|
|
SWIM
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 970
Registered: 3-9-2017
Member Is Offline
|
|
What you're describing sounds kinda like mossy zinc.
It's mostly rounded lumps that have a large surface area due to the way they're made. I believe they are slightly porous.
They vary in size from quite small to several times the size of a peppercorn.
Could it be some of that mis-labeled?
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
No, my zinc powder has the same thing. Mossy zinc is pretty distinct and quite different.
I suspect the chunks are powder that got fused together during packaging or storage. The powder at the bottom of the barrel would be pressed together
by the weight of everything above it, and a soft metal like zinc might "cold sinter" together into lumps. That's the theory, anyway.
|
|
Abromination
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 432
Registered: 10-7-2018
Location: Alaska
Member Is Offline
Mood: 1,4 tar
|
|
Quote: Originally posted by stygian ![](images/xpblue/lastpost.gif) | "is zinc malleable" - "Zinc is a bluish-white metal with a shiny surface. It is neither ductile nor malleable at room temperature."
|
I would like to disagree on the malleability statement. Although quite brittle at ST&P, you will still find zinc decently malleable. It still will
bend and can be pounded at least a bit before cracking.
It is also not common to see the true color of zinc as it instantly oxidizes instantly on contact with air.
List of materials made by ScienceMadness.org users:
https://docs.google.com/spreadsheets/d/1nmJ8uq-h4IkXPxD5svnT...
--------------------------------
Elements Collected: H, Li, B, C, N, O, Mg, Al, Si, P, S, Fe, Ni, Cu, Zn, Ag, I, Au, Pb, Bi, Am
Last Acquired: B
Next: Na
--------------
|
|