Al Powder As A Sensitizer For Nitromethane
In case anyone's interested, US Patent #6960267 teaches the use of stearic acid coated aluminum powder as a sensitizer for nitromethane.
Attachment: 6960267.pdf (608kB) This file has been downloaded 817 times
|
|
rot
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 62
Registered: 26-1-2006
Member Is Offline
Mood: No Mood
|
|
I don't think this will work because the aluminum powder would sink to the bottom of the liquid nitromethane.
|
|
jpsmith123
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 764
Registered: 24-6-2005
Member Is Offline
Mood: No Mood
|
|
The inventor addresses this issue in the patent. Supposedly the mixture will remain homogeneous for several hours (after being shaken), and if need be
can be kept that way indefinitely by adding thickeners to the mixture.
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
If particle size is tiny enough, then brownian move may help keeping the solid suspended in the liquid....
The fact it deals with Aluminium is a help because of its low density...
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|