nelsonB
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 5-9-2013
Member Is Offline
Mood: No Mood
|
|
Safely storing Diethyl ether
Hi
i was wondering if a steel F-style jugs with some sodium hydroxide to prevent peroxide formation would be enought for ether. if no tell me what would
be your idea.
![](https://cdn.discordapp.com/attachments/292782044776235018/564526270990254099/unknown.png)
[Edited on 7-4-2019 by nelsonB]
|
|
happyfooddance
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 530
Registered: 9-11-2017
Location: Los Angeles, Ca.
Member Is Offline
Mood: No Mood
|
|
If you can store it in a freezer it helps. I would be cautious about metal-on-metal lids, I might be wrong but I feel that would perhaps ignite trace
peroxides (which form on threads/parts exposed to air) more easily than glass or plastics/ptfe.
But I have stored bottles of ether for years in the freezer without problems. The ether was freshly distilled before storage, however, but without
stabilizer.
|
|
DavidJR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
Add a stabilizer like BHT.
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3027
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Or a bit of ethanol, should work as long as you don't want to do Grignards with it.
http://www.sciencemadness.org/talk/viewthread.php?tid=145410
|
|
DavidJR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
I'm not convinced that ethanol would be effective in preventing peroxide formation and even if it is, addition of ethanol severely limits what you can
do with the ether.
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Does the BHT interfere with some reactions? Does the solvent need to be distilled to remove it, before use?
In my case, I have tetralin that I wanted to use for the Mg-catalyzed potassium synthesis. I bought BHT for storing it, but haven't added it yet. I
hear this particular peroxide is pretty benign?
|
|
Mr. Rogers
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 184
Registered: 30-10-2017
Location: Ammonia Avenue
Member Is Offline
Mood: No Mood
|
|
The best way I think, is to buy several small bottles rather than one large one, and keep them in a freezer. I wouldn't feel comfortable storing a
gallon of ether in a paint can like that honestly.
|
|
Mr. Rogers
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 184
Registered: 30-10-2017
Location: Ammonia Avenue
Member Is Offline
Mood: No Mood
|
|
You can get Et2O in small quantities in Al bottles with two piece caps that come hermetically sealed. I think that's the best way to store it if you
have to.
|
|
DavidJR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
Quote: Originally posted by MrHomeScientist ![](images/xpblue/lastpost.gif) | Does the BHT interfere with some reactions? Does the solvent need to be distilled to remove it, before use?
In my case, I have tetralin that I wanted to use for the Mg-catalyzed potassium synthesis. I bought BHT for storing it, but haven't added it yet. I
hear this particular peroxide is pretty benign? |
Theoretically it could do, but the concentration required to stabilise it is pretty damn low, so it's rarely a problem. Also consider that the
peroxides, aside from being a safety concern, can potentially interfere in some reactions.
|
|