Rsambo
Harmless
Posts: 14
Registered: 9-6-2016
Member Is Offline
Mood: No Mood
|
|
Help with storage
Would somebody be able to advise me if this type of bottle is suitable for longterm storage of 70% nitric acid / 98% sulfuric acid.
https://www.ebay.co.uk/itm/MESE-Reagent-Bottle-100-250-500-1...
i've seen the PTFE capped bottles on breckland scientific but they are hugely expensive. Does anyone have any suggestions?
thanks very much.
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2690
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
The blue cap on this media bottle is polypropylene, might not last long. A glass stoppered reagent bottle might be safer and would vent any fumes if
pressure builds up. Either way I would be careful of storing that mixture for long terms.
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 514
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
In my experience PP handles 98% sulfuric acid very well, I have the same media bottles and the caps are fine after 3 years of storage. PP handles 70%
nitric acid reasonably well as well, the insides of my caps are bleached white but they are still hold strong. Maybe get a few extra caps to replace
after a few years.
One thing to note is that some of those amber media bottles are actually clear glass bottles with an amber coating of some kind. This coating flakes
off after exposure to acid fumes for a while. The ones you linked to look like genuine amber glass ones so you should be fine.
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
I wouldnt use PP for nitric acid but it's perfectly fine for sulphuric acid.
My red PTFE Duran caps didnt like nitric acid so I went for Duran Premium. After 3-4 years they are all perfectly usable
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3634
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
so far I have found that
69% Nitric acid stores well (at least a few years) in hdpe bottles with hdpe tops,
96% sulphuric acid does not escape much from hdpe bottles with caps,
but it does slowly discolour towards brown,
and the outside surface of the hdpe bottle gets 'dusty/crumbly' after a few years
(I think that the sulphuric acid VERY slowly creeps/diffuses through pores in the hdpe bottle wall ?)
whereas stored in glass it stays transparent and colourles.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Rsambo
Harmless
Posts: 14
Registered: 9-6-2016
Member Is Offline
Mood: No Mood
|
|
Thanks so much everyone. That's really helpful. I'll definitely get some and see how they fair short term and let you know. Could really do with
some ptfe caps I think for the nitric acid...
|
|
draculic acid69
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
The nitric and sulfuric I get come in the same type of bottle and if I had to store that combo I'd just use the sulfuric acid bottle.
|
|
nimgoldman
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 303
Registered: 11-6-2018
Member Is Offline
|
|
I never had any problems with sulfuric using PP cap.
I purchased two PBT caps with PTFE liner from Duran especially for HNO3 and HBr.
Note that HNO3 will leak slightly even with this cap.
There are even more expensive PFA caps, there are all-fluoropolymer, but these I think are suitable only if you frequently use them, autoclave them
and there is a risk of breaking (since Teflon is not very resistant mechanically).
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
If present on your bottle remove the pouring ring.
I destroyed one of those red caps because the pouring ring was letting vapors out.
Vapors did nothing to the PTFE liner but the cap itself...
|
|