nikotyna1939
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 59
Registered: 26-9-2018
Location: reverse poland flag or nusantara
Member Is Offline
Mood: THINK 3R REDUCE REUSE RECYCLE
|
|
synthesis of Poly(methyl methacrylate)
can anybody show me the synthesis of Poly(methyl methacrylate)
i just want to know what is the easiest route to synthesize acrylic glass
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
https://www.ebay.co.uk/itm/MOULDCRAFT-250g-WATER-CLEAR-CASTI...
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
SWIM
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 970
Registered: 3-9-2017
Member Is Offline
|
|
Nice synthesis.
I'm going down to McDonald's now to synthesize a hamburger.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Check the posts of nikotyna1939 and you will appreciate my answer,
but you are correct, I was too terse with my answer,
I look forward to reading SWIMs guidance of nikotyna1939 to synthesise PMMA at home ... should be entertaining...
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2689
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
If you depolymerize some acrylic by distilling the methyl methacrylate, and then pour it into a mold, it will eventually harden on its own into a nice
clear solid, as it will not have any inhibitors present. Otherwise a trace of benzoyl peroxide will work, maybe even the material from acne cream
would work, or you could treat the monomer with it and then decant the liquid off to remove the cream.
But any free radical source will work, hard UV lamps, ozone, peroxides, leftists, azos, or some tin salts.
|
|
Heptylene
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 319
Registered: 22-10-2016
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Dr.Bob ![](images/xpblue/lastpost.gif) |
But any free radical source will work, hard UV lamps, ozone, peroxides, leftists, azos, or some tin salts. |
Is this an attempt to initiate a political argument? ![;)](./images/smilies/wink.gif)
More seriously, have you heard of any attempt at distilling MMA from PMMA? I know styrene can be easily obtained from polystyrene and this has been
documented previously.
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2689
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
It was a pretty bad joke, only beat by yours... A
nd I distilled MMA from PMMA back in the 1980's and then repolymerizied it. I did not have any peroxides so I just lt it sit for a week or so, and
it eventually hardened. I think the experiment was right out of an organic books from the 70's. I grew up in the 70's and remember the original
radicals left over from Woodstock, but sadly was too young to go there. But it is a great way to get monomer for making acrylic.
[Edited on 25-3-2019 by Dr.Bob]
|
|
zed
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Ummm. I'll check my old chem texts. I'll try to provide a reference. Seems to me it was a common experiment, back in the 60s or 70s.
Now of course, when someone has challenged me regarding the process, the required book lies lost somewhere in my storage catacombs.
Might be "Laboratory Experiments in Organic Chemistry" by Adams.
I once had alternate synthetic uses of Methyl Methacrylate.
https://www.sciencemadness.org/whisper/viewthread.php?tid=14...
[Edited on 27-3-2019 by zed]
[Edited on 27-3-2019 by zed]
|
|
Texium
|
Thread Moved 13-3-2024 at 05:21 |