Mystery black goop from lead acetate synth
I been making Lead acetate from my concentrated Acetic acid and 35% Hydrogen peroxide using old battery terminal, this will usually be an Antimony
Lead alloy.
At first I thought it may be un reacted lead, so to test I added it to a small amount of fresh Acetic Acid and Peroxide, and nothing happened, upon
heating I got some white oxides to form but nothing much else.
I suspected the black goo would be the Antimony but every thing says its acetate / oxide should be white.
This (The Lead Acetate) will be used for making my Lead Styphnate.
That Synth went wonderfully!
![20190304_183724.jpg - 232kB](https://www.sciencemadness.org/whisper/files.php?pid=604457&aid=74170)
[Edited on 5-3-2019 by XeonTheMGPony]
[Edited on 5-3-2019 by XeonTheMGPony]
|
|
RogueRose
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1590
Registered: 16-6-2014
Member Is Offline
|
|
Carbon?
https://en.wikipedia.org/wiki/Lead%E2%80%93acid_battery#Plat...
Read 4-5 paragraphs down where it says this:
Quote: |
Modern-day paste contains carbon black, blanc fixe (barium sulfate) and lignosulfonate. The blanc fixe acts as a seed crystal for the lead–to–lead
sulfate reaction. The blanc fixe must be fully dispersed in the paste in order for it to be effective.
|
https://en.wikipedia.org/wiki/Carbon_black
|
|
XeonTheMGPony
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1640
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
I'm not using the plates for that reason, this is the thing that clamps to the wire and the post, nothing internal to the battery.
- the screws and nuts obviously lol
![18482_237202.jpg - 136kB](https://www.sciencemadness.org/whisper/files.php?pid=604490&aid=74174)
[Edited on 5-3-2019 by XeonTheMGPony]
[Edited on 5-3-2019 by XeonTheMGPony]
|
|
XeonTheMGPony
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1640
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
Gifted with another mystery of the white powder, Will not dissolve in either water or methanol, does not seem to mind nitric acid even at near boiling
temps
I started Calcining some will report back when don.
But I amp stumped, yet to try HCl.
|
|