Author: Subject: Recovery of Cesium salts from Pollucite ore.
BromicAcid
International Hazard
*****




Posts: 3254
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 1-8-2004 at 19:00
Recovery of Cesium salts from Pollucite ore.


Cesium salts are expensive and that is the limiting factor to my involvement with this alkali metal. But I found a simple method to extract relatively high purity cesium salt from its chief ore pollucite. If only I had a source for pollucite, might have to go rock hunting, but I digress.

Procedure from the series entitled "Inorganic Syntheses":
Quote:

Cesium Alum Method
Submitted By Robert West and Robert P. Anderson
Checked by Lewis I. Krimen and Therald Moeller

Pollucite is broken into pea sized lumps with a hammer and then ground in a ball mill until fine enough to pass though a 120-mesh sieve. One hundred grams of screened pollucite is mixed with 400 ml of 50% sulfuric acid (7.1 M) in a 1-L round-bottomed flask and refluxed gently for 30 hours. The mixture is diluted with 250 ml of water, heated to boiling, and filtered with suction, using a large, coarse, sintered-glass funnel. The silica residue is washed well with hot water.

The hot solution is cooled to 0C, and the well-defined octahedra of cesium alum are collected on a sintered-glass funnel and washed with cold water. A small second crop of crystals is obtained when the filtrate is concentrated to about 450 ml and cooled. The yield is about 110 g., or nearly 90% (for Varutarask pollucite).
Properties

Cesium alum crystallizes in colorless octahedra which melt at 117 C. This compound is more insoluble then the other alkali-metal alums and is remarkable for its high temperature coefficient of solubility. At 100C, 12 is soluble in 100 g of water; at 0C, only .19 g is soluble. Because of this property, the cesium compound is readily prepared in a high state of purity by recyrstalizing it from water.


An interesting and straight foreward procedure.




Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 2-8-2004 at 15:37


I also like the idea of extracting metals from ores - it is just so fundamental.

If you don't want to invest in a ball mill you can buy an 8 oz capacity iron mortar & pestle for <$30 at http://www.minerox.com/ I have one and it did a nice job of pulverizing a 1/2" piece of gravel from my driveway.

[Edited on 2-8-2004 by Magpie]
View user's profile View All Posts By User
JohnWW
International Hazard
*****




Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline

Mood: No Mood

[*] posted on 3-8-2004 at 02:39
Re: Caesium


Pollucite, the principal (silicate) ore of Cs mentioned, is itself of fairly rare occurrence.

How about looking at the possibility of extracting Cs from sea-water? I think that, like Li and Rb, it occurs in sea-water at about 1 ppm levels. Of course, as an alkali metal, its occurrence there is greatly surpassed by the Na and K. Like Li, it could conceivably be extracted, along with Rb, from sea-water with some sort of ion-exchange resin, from which, when packed in a column, the much larger fractions containing all the Na and K could be discarded.

Although the physiological action of Cs and Rb in plants is similar to that of K, which is essential to and concentrated by plants, there may be some plant species which selectively absorb Cs and Rb in preference to K.

John W.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 5-8-2004 at 13:28


If this table http://www.seafriends.org.nz/oceano/seawater.htm
is right, then the concentration is 0.0003 ppm. That means that for each gram of Cs you need about 3000 tons of seawater.
Have you got a big bucket?
View user's profile View All Posts By User
JohnWW
International Hazard
*****




Posts: 2849
Registered: 27-7-2004
Location: New Zealand
Member Is Offline

Mood: No Mood

[*] posted on 10-8-2004 at 14:19
Cs and Rb in seawater


3 grams of Cs in 3000 tonnes may not sound much, if you have read it correctly, but with sufficiently large and efficient pumps, and sufficiently efficient ion exchange resins (if they could be found) to separate Cs and Rb from the Na and K, it should be feasible. I have heard of plans to extract elements like Au and Th, found in even lesser concentration, from sea-water, and of ion-exchange separation already being used to obtain Li from sea-water.

John W.
View user's profile View All Posts By User
Polverone
Now celebrating 21 years of madness
*********




Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline

Mood: Waiting for spring

[*] posted on 10-8-2004 at 15:01


So are there any operations where you're already processing seawater on vast scales and could get additional minerals as an almost-freebie? The closest I know of is the extraction of bromine from seawater, but bromine is far more abundant than cesium. I've read of pilot-scale Japanese efforts to extract lithium, uranium, and vanadium from seawater, various schemes ranging from really-kooky to conceivable for gold from seawater, and proposals for other metals, but nothing that's reached full-scale production.



PGP Key and corresponding e-mail address
View user's profile Visit user's homepage View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 14-8-2004 at 04:33


Lithium is about 7 times as expensive as cesium and about 500 times more common in sea water.
There is a real demand for lithium for industrial purposes and for the nuclear and pharmaceutical business. There is also a real demand for bromine, perhaps less so than when it was added to leaded petrol, but real.
The demand for cesium is a few chemists in research labs and a few physicists with clocks. If you were able to double the world's supply of cesium you would pretty much halve the price.

I don't think the ecconomics don't make sense.
Also, if I shift that 3000 tonnes of water I can hope to extract a gram of the stuff., worth about £0.82 which would buy me about 40 KWh of energy (based on my gas bill). I'm not sure that 40Kw would process 3000 tonnes in an hour, its only enough to lift the water about 15 feet clear of sealevel.

[Edited on 14-8-2004 by unionised]
View user's profile View All Posts By User
Polverone
Now celebrating 21 years of madness
*********




Posts: 3186
Registered: 19-5-2002
Location: The Sunny Pacific Northwest
Member Is Offline

Mood: Waiting for spring

[*] posted on 14-8-2004 at 11:40


Lithium is more expensive than cesium?! Either you've found a great bargain-basement cesium compounds dealer or you're paying too much for lithium compounds!

For example, Aldrich wants $35.10 for 500 g of 99% lithium carbonate and $99.50 for 250 g of 99% cesium carbonate. The price differential is much smaller with highly-purified materials, presumably because the price of purification is large compared to the price of raw materials.

You can buy technical grade lithium carbonate (for pottery) for less than $16/kg. I've never found any cesium compound of any grade for sale near that price.




PGP Key and corresponding e-mail address
View user's profile Visit user's homepage View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3254
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 14-8-2004 at 17:31


One biochemistry web site sold cesium chloride for the unbelievable price of $175 a kilogram, that for me was pretty cheap.

BTW, I read recently that lithium is one of only two metals that has actually increased in price (when leveled with the consumers price index) over the last twenty or so years, probably due to the difficulty of processing ore and the highly increasing demand for it.




Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 17-8-2004 at 08:18


"Lithium is more expensive than cesium?! Either you've found a great bargain-basement cesium compounds dealer or you're paying too much for lithium compounds! "
Or I goofed, and got them the wrong way round.:(
The point is that cesium is rare and almost useless so it's expensive.
The concentration in the earth's crust is estimated as 27 ppm so you would do better picking up a random rock rather than the same weight of seawater. (though, I realise the rock would be harder to process).
View user's profile View All Posts By User
halogen
Hazard to Others
***




Posts: 372
Registered: 18-4-2004
Member Is Offline

Mood: No Mood

[*] posted on 17-8-2004 at 08:57


Steps for mining oceanic materials::D
1. Create nuclear reactor and steadily improve it until tremendous power output.
2. Buy a few tons of freshly evaporated sea salt, seaweed, and such.
3. Perform a massive electrolysis!
4. Separate the halogens and similar materials and sift through the metal.
5. Sell the metallic parts or save some, and keep the tanks of precious fluorine, chlorine, bromine... and I dont really think you can put iodine in a tank...
6. Use money to uprade reactor and buy raw sea materials. (Repeat)
7. Repeat until you have all the metals and halogens and chemicals and money you need.
------------------------------------
Yes... I have gone mad...
:P




F. de Lalande and M. Prud'homme showed that a mixture of boric oxide and sodium chloride is decomposed in a stream of dry air or oxygen at a red heat with the evolution of chlorine.
View user's profile View All Posts By User
rift valley
Hazard to Others
***




Posts: 103
Registered: 24-7-2004
Location: NH
Member Is Offline

Mood: semiconducting

[*] posted on 17-8-2004 at 09:46


Hmmm. Back in the late 1800's and early 1900's they were various pollucite ore mines in nearby Maine. In the last weeks of summer maybe I'll take a trip over there and see what I can find.
View user's profile View All Posts By User
vulture
Forum Gatekeeper
*****




Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 17-8-2004 at 10:54


According to Römmp, seawater contains about 1 microgram of Cs per liter.

When Bunsen and Kirchhoff (sic) extracted it from Bad Dürkheimer (Germany, Eiffel) mineralwater they needed about 42000L to produce a few grams IIRC. And that water is supposed to be enriched with it because of vulcanic activity...




One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 17-8-2004 at 14:41


I don't supose it matters much if it's 1 gram in 1000 tonnes or 1 gram in 3000 tonnes.
A few grams in just 42 tonnes is a lot better, but I'm glad I didn't have to do that experiment.
View user's profile View All Posts By User
lacrima97
Hazard to Self
**




Posts: 93
Registered: 24-7-2005
Location: MS
Member Is Offline

Mood: experimental

[*] posted on 10-2-2006 at 20:40


Does anyone know of any sources of pure cesium?
View user's profile View All Posts By User This user has MSN Messenger
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 10-2-2006 at 20:57


This sounds like it should be in a new thread.

Are you looking for a cesium salt or the metal itself? If you're looking for the metal, look for chemical suppliers (very expensive), element suppliers (less expensive) and eBay.
View user's profile View All Posts By User
lacrima97
Hazard to Self
**




Posts: 93
Registered: 24-7-2005
Location: MS
Member Is Offline

Mood: experimental

[*] posted on 10-2-2006 at 21:13


Yeah, I have noticed that the pure metal (what I want) is extremely expensive. I believe that electrolysis of a cesium compound is out of the question, so I am going to just rid myself of the idea. I have nor the money for the pure metal, nor the stupidity to electrolize such a metal.

By stupidity, I mean with my equipment.
View user's profile View All Posts By User This user has MSN Messenger
woelen
Super Administrator
*********




Posts: 8032
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 11-2-2006 at 05:15


And what kind of experiments did you have in mind for the elemental cesium? The stuff is so reactive (e.g. explodes in contact with water, inflames in air), how would you manage to keep it around without causing accidents?



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 11-2-2006 at 08:25


Store it under mineral oil?

Bromic's patent for making sodium in the 'unconventional sodium' thread also includes an easy synthesis for elemental Cs. Keep in mind though that no one here has gotten the processes in that patent to work yet. We're still trying to figure it out.
View user's profile View All Posts By User
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 11-2-2006 at 11:26


Cs is just so reactive I would likely not feel comforatble working with it at home without an inert gas atmosphere glovebox. Cesium hydroxide is so corrosive that if your cesium were to react with air or water accidently you would have a nasty spill on your hands.

If I get this summer research scholarship I applied for I will get to play with elemental cesium and other lower alkalis to make alkali mercurides and aurides.:cool::cool:




View user's profile View All Posts By User
olmpiad
Harmless
*




Posts: 29
Registered: 2-6-2006
Location: this thing known as earth
Member Is Offline

Mood: Dandy

[*] posted on 6-2-2007 at 20:15


I did the procedure as first stated, but reduced everything to 10% of the original weights. It actually works quite well, and the Cs-Alum forms very quickly by placing the solution in a fridge (after about four hours of decanting). Ill post pictures soon. They crystals do not look too much different than normal alum, but their solubility is a dead give away. First Cs salt I've ever made, and it was quite a success! Ill post pictures soon.

[Edited on 2/7/07 by olmpiad]




View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 8-2-2007 at 03:11


Where did you get the ore from?
View user's profile View All Posts By User
olmpiad
Harmless
*




Posts: 29
Registered: 2-6-2006
Location: this thing known as earth
Member Is Offline

Mood: Dandy

[*] posted on 10-2-2007 at 14:54


Picture:

Unionized:
i got the Pollucite from my mineral collection (minerals are my passion), It is from a rare locality in California.




View user's profile View All Posts By User
pantone159
National Hazard
****




Posts: 590
Registered: 27-6-2006
Location: Austin, TX, USA
Member Is Offline

Mood: desperate for shade

[*] posted on 10-2-2007 at 16:00


One link offering to sell pollucite samples, $25...
It doesn't say how much, though.

http://www.sciencemall-usa.com/polcesmin.html
View user's profile Visit user's homepage View All Posts By User
olmpiad
Harmless
*




Posts: 29
Registered: 2-6-2006
Location: this thing known as earth
Member Is Offline

Mood: Dandy

[*] posted on 13-2-2007 at 17:14


I find that quite expensive. The site says that the specimen comes in a Perky Box, which means that it is a TN specimen. As for size reference, this is known as a Thumbnail to us mineral collectors, which is exactly what it sounds like: the size of your thumbnail. In other words, probably no more than 5g, and it cost 25$. I paid $7 for my specimen, and it is a C (for those of you who do not collect minerals, this is known as a Cabinet size), and it weighs a good 500-600g.



View user's profile View All Posts By User