What material should be used as a vacuum seal?
I need a sheet of a rubber like material to be used between two surfaces to form a vacuum seal. The surface is an acrylic cylinder and two acrylic
disks on either side. So the material needs to go between the lip of the cylinder and the disks to seal it when a vacuum is applied.
Does anyone know what kind of material is best? I need to buy it as a sheet and cut it to the right size.'
Also sorry for my previous posts I've been diagnosed with schizoaffective disorder and gone on medication for almost a year and it seems to have
helped me out a lot.
I am a buttmeister
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
neoprene rubber sheet should work for you
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Silicone's another good option (get the softer stuff, obviously). Pretty sure you can buy sheets as some sort of kitchen accessory?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1314
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Neoprene is better than silicone. The gas permeability of silicone is surprisingly high. I make a product that uses silicone tube as a gas diffusion
membrane. That may or may not matter in your application of course.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
SWIM
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 970
Registered: 3-9-2017
Member Is Offline
|
|
Neoprene is what they used to use as a seal in old-style Virtis lyophilizer flasks , and high vac is the whole point with those babies so it must work
well.
If you only need one open end, you might be able to bond the other end on with some monomer based adhesive instead of using a gasket. I know this can
be done with plexiglass, but don't know much about acrylic.
This ought to result in a stronger vac chamber if its doable.
|
|
AdamAlden
I have a theory about life, the universe and everything.
![*](images/xpblue/star.gif)
Posts: 91
Registered: 18-3-2016
Location: California
Member Is Offline
Mood: Radioactive
|
|
Neoprene looks kind of stiff or tough but it should still make a good seal with some pressure applied. Thanks for advice guys I'll give it a try.
I am a buttmeister
|
|
XeonTheMGPony
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1640
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
use a silicone based lube, Vitron is my general go to due to its fairly good chemical compatibility
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3649
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Although silicone rubbers are more porous than natural rubber or many synthetic rubbers,
it is a good choice because - it is cheap and it works.
Chemical resistance is good,
you probably will not notice the porosity unless you are going for high vacuum.
Have you calculated the force on the end disks ?
I worry sometimes when I see YT videos of folks applying vacuum to large thin acrylic disks.