Pt is widely know for catalyzing many reactions, especially with H2. My question is what makes it such a good catalyst? My chem teacher didn't know why. I searched google and didn't find any explanation. I did however find that H2 can form complexes with metals. Is this the main reason for catalystic properties of Pt metals? But then, why don't other transition metals catalyze H2 reactions if they all have the ability to adsorb H2?



View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1306
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 7-2-2006 at 19:03


Nickel will catalyse hydrogenation reactions. But Pt is better at it. Why? I don't know.



Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 7-2-2006 at 19:21


IIRC catalysts work by providing a reaction route that requires less energy. I don't know the mechanics for how Pt works, however.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
guy
National Hazard
****




Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline

Mood: Catalytic!

[*] posted on 7-2-2006 at 19:49


I found a site(http://www.science.uwaterloo.ca/~cchieh/cact/applychem/heter...) that describes a little about how it works. All it said was that the Pt adsorbs H2 and weakens the bonds.
It said other metals may attract H2 too much and not make the reaction work. Some how it said that metals farther left are stronger chemisorbers. Why? they have larger radius and smaller electron affinity.




View user's profile View All Posts By User
guy
National Hazard
****




Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline

Mood: Catalytic!

[*] posted on 9-2-2006 at 17:04


This site better explains how hydrogen is chemisorbed to Pt.
http://www.library.uu.nl/digiarchief/dip/diss/2002-1028-1505...




View user's profile View All Posts By User
mick
Hazard to Others
***




Posts: 338
Registered: 3-10-2003
Member Is Offline

Mood: No Mood

[*] posted on 13-2-2006 at 13:25


Catalytic hydrogenation is a 3 phase reaction. Gas, liquid and solid. The solid adsorbs the gas and the liquid makes it work.