Starlite as high temp insulation material ?
I found on this Youtube channel that Starlite is invented as a very high temperature resistant material invented by a British chemist, but it is never
published or patented and the inventor has deceased without revealing any details.
https://en.wikipedia.org/wiki/Starlite
But a compatible stuff can be made with starch, baking soda and glue.
Nighthawkinglight showerd how to make it:
https://www.youtube.com/watch?v=aqR4_UoBIzY
Here experiments of Beyond the Press:
Against oxyacetylene burner:
https://www.youtube.com/watch?v=0anEMZs9zHE
Against plasma cutter:
https://www.youtube.com/watch?v=7wvTXDjwrLI
This would be an excellent furnace insulator. Did anyone experiment with it ?
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
good insulator, but not good for a furnace lining. the carhon foam it creates will eventually be burned buy the prolonged fire in a furnace, we are
not talking of minutes, but probably days of firing. carbonized bread is also a good insulator, there's a post here somewhere, still carbon foam
though
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
mayko
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1218
Registered: 17-1-2013
Location: Carrboro, NC
Member Is Offline
Mood: anomalous (Euclid class)
|
|
Yup! I still have a couple of pieces:
https://www.sciencemadness.org/whisper/viewthread.php?tid=84...
al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
|
|
Texium
|
Thread Moved 29-11-2023 at 11:47 |