£3.53 frit Buchner Funnel eBay
EBay UK has some cheap Buchner funnels and the ones I received were good quality for the price. No ground glass joint and only 30ml and 60ml for
£3.53 free postage The 30 ml is a little cheaper frits G1 to G5. They are from Chine so they can take a couple of months to arrive.
Item: 33225099313
Borosilicate glass:
Good temperature resistance and good thermal shock resistance but finite.
For normal, standard service typically 200-230°C, for short-term (minutes) service max 400°C
Maximum thermal shock resistance is 160°C
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
https://rover.ebay.com/rover/0/0/0?mpre=https%3A%2F%2Fwww.eb...
same item but cheaper
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
It looks about the same except for the 60ml G4 (the popular grade) is almost twice the price at $7. It does depend on the on the $ to £ exchange
rate and they don't say postage is included and that they do not deliver to the UK where I am.
Borosilicate glass:
Good temperature resistance and good thermal shock resistance but finite.
For normal, standard service typically 200-230°C, for short-term (minutes) service max 400°C
Maximum thermal shock resistance is 160°C
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3646
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Pity they do not have ground joints.
it may be worth geting a buying a full set ?
eBay uk has listings for sets of five
35ml £9.60/set https://www.ebay.co.uk/itm/Set-of-5x-Pore-Size-G1-G5-Glass-B...
60ml £12.72/set https://www.ebay.co.uk/itm/Set-of-5x-Glass-Buchner-Funnels-w...
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
Nice find I paid almost that for three. Yes I would have got the full set. I don't have much use for the G1 and G2 but at that price having them would
have been nice and I could use them with filter paper if I needed to. Now I just need to find cheap rubber or silicone bungs that fit my flasks. I
object to paying more for the bung than the Buchner LOL
Borosilicate glass:
Good temperature resistance and good thermal shock resistance but finite.
For normal, standard service typically 200-230°C, for short-term (minutes) service max 400°C
Maximum thermal shock resistance is 160°C
|
|