Iridium
I want to do a little experimenting with this fascinating metal, but I have run into a problem: I can't find it for a decent price. The current spot
price is $6.27USD/gram, but the cheapest I have been able to find it is $16/gram + $25 shipping and this was on eBay! The Thomas Register doesn't list
any better sources, nor does froogle. I won't even mention chemical suppliers' prices...
What's the cheapest way to get a couple of grams of iridium? (The physical form doesn't matter.) I've come up with nothing here and will gladly take
any suggestions.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
What kind of expriments are you thinking of with the iridium? I have a source in Germany for powdered iridium at EUR 8 per gram (appr. $10 per gram),
minimum offtake 5 grams, but I did not buy it yet, because I have not found any way to chemically dissolve this metal. If I just have some powder,
which does not dissolve in anything, then of course, it is not worth the money.
If you wish, I can lookup that source for you. One year ago, I purchased 5 grams of ruthenium powder as well from that source for appr. $8 per gram. I
do not know, however, what shippings costs you will have (I live in the Netherlands, next to Germany, so I only had to pay EUR 2 or something like
that for postage, for you it will be more, due to overseas shipping). With the ruthenium I indeed have done very interesting experiments, some of
these are on my website with pictures.
These spot prices, you mention for the noble metals, usually are for large quantities (at least one ounce or something like that). Smaller quantities
become progressively more expensive.
So, if you know of a method to dissolve the metal chemically in an aqueous solution (not a molten alkali, for that I have no safe possibilities where
I live), then I would be very pleased.
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
I was going to try some things to dissolve the stuff. Fenton's reagent (pH 3) + chloride was first on that list, then maybe persulfate (acidic, if
possible) + chloride. Nitrate + hydroxide in a nickel crucible if all that failed... It's worth a try.
How old is that price? I know that precious metal prices fluxuate wildly.
|
|
Eclectic
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 899
Registered: 14-11-2004
Member Is Offline
Mood: Obsessive
|
|
The current spot price is about $200 per try oz. (about 31g).
I had to buy 5 oz @$225/oz for my experiments in recreating the One True Ring. Since I don't have access to the fires of Mount Doom, I'll have to use
an electric arc.
As far as I've been able to determine, Ir is imperveous to ALL acids, including HF/HNO3 and aqua regia. It will react with molten sodium peroxide and
then with HCl to form the chloride.
|
|
Sergei_Eisenstein
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 290
Registered: 13-12-2004
Location: Waziristan
Member Is Offline
Mood: training
|
|
Quote: | Originally posted by Eclectic As far as I've been able to determine, Ir is imperveous to ALL acids, including HF/HNO3 and aqua regia. It
will react with molten sodium peroxide and then with HCl to form the chloride. |
Iridium catalysts are made from either Ir(III) acetate or IrCl3.xH2O, the latter being used as precursor for many ligand Ir complexes (COD, Ph3P,
...). Ir(III) acetate is made by reacting iridium metal with barium peroxide in the presence of EtOH/HOAc at very high temperatures. To make Ir(III)
chloride hydrate salts, iridium metals is fused with NaCl under an atmosphere of Cl2 at very high temperature, and the cake is dissolved in water. The
Ir salt is precipitated by addition of NH4Cl and treated with aqua regia. Reducing this solution in volume will give you IrCl3.xH2O
Overview of possibilities:
![](http://img437.imageshack.us/img437/7145/ircat8qt.gif)
Reference: PB Kettler. Platinum Group Metals in Catalysis: Fabrication of Catalysts and Catalyst Precursors. Org Proc Res Dev 7 (2003)
342-354
I agree there are easier precious metals to start playing with For sources, it
might be possible to check out specialized gold and silver dealers. They also sell platina and palladium, and may have access to iridium, rhodium and
ruthenium. These metals are used in the electronics industry as well, and you can find companies specialized in recuperation of the precious metals
from old electronic equipment. Drawback is you often have to order no less than 1 kg, but if you have a chemical company, this clearly is the way to
walk.
|
|
garage chemist
chemical wizard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1803
Registered: 16-8-2004
Location: Germany
Member Is Offline
Mood: No Mood
|
|
@ woelen:
Hollemann- Wiberg states that the best solvent for Iridium is a hot mixture of conc. HCl and NaClO3.
Iridium begins to oxidise in air at 700°C forming volatile IrO3.
For working with hot iridium, inert gas atmosphere or vacuum must therefore be used.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
The price I quoted is around one year old. Indeed, prices of the precious metals fluctuate wildly, but I think that the price of iridium still will be
something like that.
With the ruthenium I have, I also tried the method conc. HCl + NaClO3. Someone on usenet:sci.chem told me, but it did not work at all, despite the
stories about ruthenium reacting violently or almost explosively with HCl/NaClO3. I got a lot of ClO2 and some Cl2, so indeed I could get explosions
, but still completely undissolved Ru metal. I suspect that this method also
does not work with iridium.
Someone else on usenet:sci.chem (Farooq) told me to use an alkaline solution of NaClO and boil the solution with the ruthenium powder in it. That
worked like a charm. Within minutes, the powder was dissolved. However, this method does not work with iridium as stated by multiple people on other
forums (e.g. the dutch chemieforum).
[Edited on 14-1-06 by woelen]
|
|
zoomer
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 66
Registered: 22-3-2005
Location: Watching the sun set over the saguaros
Member Is Offline
Mood: Always Curious
|
|
Johnson Matthey is used by a number of U.S. jewelers for many precious metals, including iridium. They sell Ir in sheets, disks, wire, crucibles, and
other forms:
http://www.noble.matthey.com/product/detail.asp?article=34
Their catalyst division also sells a large number of compounds of the noble metals, including most of the ones mentioned in this thread:
http://www.jmcatalysts.com/pct/marketshome.asp?marketid=79
I couldn't find any prices, though, you'd have to contact them. Ironic as it sounds, maybe a jewelry supplier might have better prices...?
Z
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
Woelen can you post the source you have for the powdered iridium?
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
An eBay seller, who had iridium and ruthenium powder, is known as [removed on request] on eBay. From him I purchased 5 grams ruthenium metal for EUR
30. He is Germany-based. His email address is [removed on request]. This person had iridium metal in the form of fine powder as well, but I did not
purchase that, because I did not know of any way to dissolve this (see previous post). This was in april 2005.
Another interesting seller was [removed on request]
I purchased 10 grams powdered rhenium metal metal from this seller one year ago. He also had iridium at that time.
This seller also is known from eBay as "smart-elements". Sometimes he has interesting things on eBay, other times nothing or just very expensive
things. Just check out.
This seller is Austria-based and he also apears to have a place in Germany, so he is most interesting for European persons.
[Edited on 3-12-07 by woelen]
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
C.W. Ammen in his book Recovery and Refining of Precious Metals describes dissolving platinum, Pd, and Ir using aqua regia.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
I have read that book front to back many times Magpie, but there exists abundant typographical errors (like any other Ammen book, good hands on
experience, but bad editing :p) so I wouldn't put too much emphasis on that procedure when later on he talks about fusing it with potassium hydroxide
and nitrate in zirconium crucible and then dissolving the fusion in water leaving IrO2 as a powder which is then dissolved in aqua regia and
precipitated with ammonium chloride. IIRC, iridium is the most corrosion resistant pure metal known to man.
Neutrino, I personally would call Johnson Matthey or Alfa Aesar (a subsidiary of the former) and inquire about it, $200/troy ounce sounds a little low
to me but I imagine it would be in that ballpark. You can buy off of ebay, but you'll pay probably the same or more and you won't have a guarantee
about purity. Cheapest thing would be to get a powder, and definitely easiest when it comes to dissolving it.
Oh, eclectic, I have no idea how you plan to fabricate yourself a ring out of it using an arc furnace but I'm interested in hearing your idea
nonetheless. I'm thinking you'll have to use an e-beam furnace to keep it molten (since at those temperatures removing the heat source=instantaneous
solidification b/c of loss to radiation) and the mold hot enough to prevent instant chilling. Additionally, what type of mold would you use? I'm
guessing sintered magnesia since graphite and SiC are out of the question because you'll get iridium carbide. Anyways, U2U me, I'd like to discuss it
![:)](./images/smilies/smile.gif)
garage chemist, this statement "Iridium begins to oxidise in air at 700°C forming volatile IrO3.
For working with hot iridium, inert gas atmosphere or vacuum must therefore be used." goes against the information found (courtesy Johnson Matthey)
here: http://www.noble.matthey.com/product/detail.asp?article=34
I always thought iridium behaved more like the oxidation-resistant platinum than osmium and ruthenium (which both form volatile, poisonous oxides,
some @ room temperature).
And from the conflicting reports of what dissolves it and what doesn't (and the limited number of us that actually have any and aren't just
speculating) it would seem that the jury is out on what works best in an aqueous environment.
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
I asked Matthey, they said they don't deal with individuals. Alfa is a chemical supplier, I don't see any point in asking them. I'll try woelen's
suppliers next.
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
I went ahead and looked through the Alfa catalog in the lab and yeah, you definitely don't want to order from them, the minimum purity Ir is about
1.7X the market value. Maybe try advent research materials or perhaps even READE: http://www.reade.com/Products/Elements/iridium.html
but I suggest you talk eclectic since he had to purchase 5 ounces of it, I'm sure he knows where to buy it (and the price he got sounds pretty fair!)
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
1.7 times the spot price? Are you sure about that? The quote I got was much more. I will have to look into this because this is the best deal I have
heard about so far.
Buying in bulk at the spot price is easy. I'm trying to <b>avoid</b> spending thousands...
Is there any particular reason you advise on those companies? Their kind usually doesn't sell to the likes of us.
|
|