Can you use Water as an eluent on an Alumina column?


Can you use Water as an eluent on an Alumina column?

The only solvent my compound is soluble in is aqueous NaOH at a pH of 10. So I'm thinking of running an alumina column and use water as eluent, will that work? Any drawbacks?
View user's profile View All Posts By User
ClF3
Harmless
*




Posts: 8
Registered: 19-10-2018
Location: The dark depths of North Wales
Member Is Offline

Mood: Nitrous Happy

[*] posted on 19-11-2018 at 01:49


Hi is the compound Fe2+ or Fe3+ ions by any chance?

[Edited on 19-11-2018 by ClF3]




--
ClF3
View user's profile View All Posts By User
beerwiz
Hazard to Others
***




Posts: 128
Registered: 6-2-2014
Member Is Offline

Mood: No Mood

[*] posted on 19-11-2018 at 21:11


Quote: Originally posted by ClF3  
Hi is the compound Fe2+ or Fe3+ ions by any chance?

[Edited on 19-11-2018 by ClF3]


No. What's your opinion, can you use water as eluent on alumina?
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 20-11-2018 at 00:12


It should be fine to elute. pH 10 isn't high enough to dissolve alumina.



As below, so above.