Author: Subject: High Temp Wire/Sparkplug sources? (1000c+)
Sidmadra
Hazard to Others
***




Posts: 129
Registered: 17-2-2017
Member Is Offline

Mood: No Mood

[*] posted on 5-11-2018 at 14:49
High Temp Wire/Sparkplug sources? (1000c+)


I'm building a furnace that I plan to use a high voltage electric sparker to ignite, but for that I need a high temp wire or sparkplug which can handle the heat once the flame gets going. I read that there are kiln wires designed for the high temps of kilns, but the only thing I am finding are nichrome wire. I don't need anything for resistive heating, but something through which a current can travel. Anyone have an idea where I can get such wire or a high temp spark plug? I'm not having luck finding any online, but I'm probably searching the wrong terms.

Basically am in need of low resistivity high temperature resistant wire.

[Edited on 5-11-2018 by Sidmadra]
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3741
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 5-11-2018 at 15:40


Can you make a spark gap using solid steel electrodes with connections outside of the oven ?
e.g. https://www.ebay.co.uk/itm/Ideal-Ignition-Electrode/32353320...
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1331
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 5-11-2018 at 16:41


FeCrAl wire on Aliexpress ("Kanthal")

I know its 'resistance'wire but it should work just fine for sparks.
It works out to about 3.5 ohm per m.




Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
weilawei
Hazard to Others
***




Posts: 130
Registered: 3-12-2017
Member Is Offline

Mood: No Mood

[*] posted on 6-11-2018 at 05:20


Steam Engine is a calculator intended for people making coils for vaporizers out of various resistance wires and diameters. That ought to help you dial it in.
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 6-11-2018 at 05:26


Smash a lightbulb?
View user's profile View All Posts By User
kulep
Harmless
*




Posts: 46
Registered: 19-5-2018
Location: Somewhere below the tropic of Capricorn
Member Is Offline

Mood: Spicy

[*] posted on 6-11-2018 at 06:28


Get a tungsten tig electrode or a tungsten rod from ebay, should handle whatever temp you achieve. You could probably use a zinc carbon battery graphite electrode but it would certainly burn out in a high temperature oxygen rich atmosphere.

As you are dealing with high voltages you don't need a low resistance material.
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 6-11-2018 at 07:35


But why not use a hot wire igniter? Small engines use glow plugs, and gas-fired central heaters use hot surface igniters. No spark necessary if the surface is hot enough.



View user's profile View All Posts By User
Jackson
Hazard to Others
***




Posts: 189
Registered: 22-5-2018
Location: U S of A
Member Is Offline

Mood: :) Happy about new glassware :)

[*] posted on 6-11-2018 at 08:54


Doesnt Nichrome and Kanthal burn out under high temps? I remember seeing something about them ablating or just permanently losing connection under high temps. I could be wrong though.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 6-11-2018 at 10:46


as kulep said tungsten is a good idea, thick tungsten. lightbulbs have the filament in a vacuum or in an inert atmosphere for a reason, the thin tungsten wire burns in air if it's glowing hot.
i have a few options in mind.
nichrome or kenthal wire eventually burns if inside a flame (furnace flame rich in oxygen or just really hot) for many hours, you did not specify what kind of furnace you are building, gas, oil or pellets powered?
i suppose you are going to use propane, as i said a hot filament directly inside the flame cone is not a good idea, but maybe a filament or spark plug just offset the flame cone should work. propane exits the torch nozzle diffusing around it, when contacts the hot filament ora spark it ignites forming the flame cone out of the nozzle, missing the filament or spark plug.
a problem of this system could be that if the air gas mixture doesn't ingnite in the first few seconds, the furnace would fill with the explosive mixture, and once lit you get the idea, like hard starts for rocket engines

[Edited on 6-11-2018 by Ubya]





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 6-11-2018 at 11:35


This is what I'm talking about, by the way.

https://www.homedepot.com/p/Emerson-Hot-Surface-Ignitor-Sili...



emerson-grow-room-ventilation-767a-373-64_1000.jpg - 41kB

There are all different sizes and prices available for these. If the furnace can be configured to use something like this, then it makes starting the flame pretty easy and reliable. They are generally made from silicon carbide or nitride.




View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1380
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 6-11-2018 at 14:02


Maybe smashing a light bulb is still not a bad idea, not for the filament, but for its support wires which are supposed to be molybdenum (mp >2600 C).

They are a bit short and thin though, a tungsten welding electrode would be more robust.




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1331
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 6-11-2018 at 14:22


Tungsten will burn up in an oxidizing atmosphere at furnace temperatures (600C+).



Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1712
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 6-11-2018 at 17:37


I remember a small toaster oven I had that jacketed the footlong heating elements in a ceramic - like a coat hanger wire in thickness and a hard white ceramic over it. Maybe something like that philosophy could work where a suitable alloy would be shielded for the most part, except for the terminal end.
If you had some ceramic tubing with a tiny hole diameter, perhaps you could retract or back off a metal or carbon electrode sleeved inside the ceramic once you spark started the oven.

[Edited on 7-11-2018 by Morgan]
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6343
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 6-11-2018 at 18:21


Well the victor apparently is hafnium.
http://theodoregray.com/periodicTable/Elements/072/index.htm...

But something prefabricated that would work well might be better. I like WGTR's idea.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1712
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 7-11-2018 at 16:45


Another idea occurred to me, something they do with pulse jets that typically use spark plugs. Aside from just torching the side of the jet to a red heat, (hot surface ignition), some just make a long spark ignitor rod and stick it up the tailpipe and once the jet starts, retract the rod. So maybe one could light the flame in the furnace and then proceed to put the top lid on or close it up, no high temperature device needed if permissible or designed for such - or have a very small access hole.

Here's a steel tube being devoured in a furnace of sorts.
https://youtube.com/watch?v=F8vqfphZ73A


[Edited on 8-11-2018 by Morgan]
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1712
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 7-11-2018 at 17:49


Hafnium tidbits

"Hafnium is subject to severe embrittlement by relatively minute amounts of impurities, especially nitrogen, oxygen, carbon, and hydrogen. They have a high affinity for these elements at the welding temperature. Because of this high affinity for gaseous elements, hafnium must either be welded using arc welding processes with inert shielding gases, such as argon or helium, or be welded in a vacuum."
https://www.eaglealloys.com/hafnium-guide/

"Although it has a melting temperature of 2230 °C it is generally considered a reactive metal rather than a refractory metal. It is subject to severe embrittlement by relatively small amounts of impurities and is rarely sintered. It is generally formed by hot-rolling between 550 and 800 °C or extrusion above 960 °C. It can be cold rolled only 15–25% between annealing treatments."
https://www.sciencedirect.com/topics/materials-science/hafni...

"A breakthrough came with the invention of the button-type electrode. The electrode, when embedded into a water-cooled copper holder, enhanced emissive element cooling. Moreover, thoriated tungsten was replaced by zirconium when the plasma forming gas was air. The electrode life increased from a few minutes with tungsten to a few hours with zirconium, and air cutting of mild steel became popular."
"However, it was practically impossible to use zirconium cathode at arc currents higher than 300 amps. At the end of the 1960s, the use of hafnium in the former Soviet Union to replace zirconium, lanthanum, and strontium further improved electrode life in air plasma cutting."
https://www.thefabricator.com/article/plasmacutting/the-life...

[Edited on 8-11-2018 by Morgan]
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2170
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 11-11-2018 at 10:00


Just buy a regular spark plug for a car. They are designed for exactly this kind of usage. 1000c is a normal temperature inside an engine cylinder at the spark plug. The cylinder walls and piston tend to be cooler but head temps at the spark plug tip are closer to adibatic.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1712
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 11-11-2018 at 11:02


I bought a few Eclipse and Auburn ignitors that have a long reach. The one on the right is an eclipse brand with a 3/4 inch pipe thread. The little plugs have a 1/4 32 inch thread for comparison.
http://www.pulse-jets.com/phpbb3/download/file.php?id=6345



[Edited on 11-11-2018 by Morgan]
View user's profile View All Posts By User