nooneshere
Harmless
Posts: 4
Registered: 25-9-2018
Member Is Offline
|
|
Fluidized drying bed
Trying to locate one of these.. seems they're all 5K used and 10-15k minimum new. A little out of my park..
there has to be some smaller scale or consumer like product like this ? or perhaps a good spot I havent found with used ones that actually have all
the parts?
alot of the used ones have no vessel / container or top for the device..
|
|
nooneshere
Harmless
Posts: 4
Registered: 25-9-2018
Member Is Offline
|
|
ive seen some " fluid air coffee roasters" but I doubt these will actually be able to handle wet clay material without flooding and short circuiting
..
any alternatives to drying wet material ? perhaps a vac oven? any input for best achieving wet material drying ..
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Forgive me, I'm not very familiar with the use of fluidized beds. Would a vacuum dessicator not suffice?
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|