What is this solid (Solved)
Hey SM,
Today I come to You with another mystery solid.
This should not be hard!
Do I got this from the same institute of Inorganic chemistry.
It is shaped like a parallelogram from the front and back and rectangle from all other sides. I got it in two forms, 2 mm and 4 mm high, and both 25
mm deep and 50 mm wide.
![1.PNG - 238kB](https://www.sciencemadness.org/whisper/files.php?pid=525148&aid=69555)
It is red-orange transparent solid with pretty low melting point. ( I thought it was just some kind of glass and for safety tried its compatibility
with heat) it melts @ about 100-200 °C (I can test for more accurate MP, if needed. )
![2.PNG - 654kB](https://www.sciencemadness.org/whisper/files.php?pid=525148&aid=69557)
when in gas flame, it gives bright blue color flame and some of solid boils and condenses as a yellow layer on solid itself.
![3.PNG - 705kB](https://www.sciencemadness.org/whisper/files.php?pid=525148&aid=69559)
It has density of about 7.35 g/ml, it feels quite heavy.
It has these markings on the side.
![4.PNG - 236kB](https://www.sciencemadness.org/whisper/files.php?pid=525148&aid=69561)
My guess was tin iodide, but it is much more dense.
Do you have any guesses? Any tests in mind?
BTW: it is not soluble in water. and it is not hard at all.
[Edited on 22-7-2018 by TheMrbunGee]
[Edited on 22-7-2018 by TheMrbunGee]
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
STOP SETTING FIRE TO RANDOM THINGS.
It's almost certainly KRS 5 which is remarkable toxic.
http://www.internationalcrystal.net/optics_17.htm
https://www.spectral-systems.com/products/krs-5-atr-optical-...
|
|
TheMrbunGee
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 364
Registered: 13-7-2016
Location: EU
Member Is Offline
Mood: Phosphorising
|
|
Yeah, I probably should! Good thing I had strong ventilation on, when I was heating it.
Looks like it really is Thallium Bromo-Iodide.
Well - I have been touching it bare handed, so I should have some prussian blue for dinner.
And I told it would be easy. not sure how did I underrated the melting point
so badly.
|
|