[*] posted on 14-5-2018 at 02:59
Removal of Na2SO4 from Mg(OH)2


After reacting MgSO4 with NaOH I want to remove the Na2SO4. I've tried filtering which was very slow and now just mixing the products with water and waiting for them to separate and then removing the clear supernatant with a turkey baster. But it takes a long time for the clear layer to appear.

Any suggestions?

Thanks.
View user's profile View All Posts By User
CobaltChloride
Hazard to Others
***




Posts: 239
Registered: 3-3-2018
Location: Romania
Member Is Offline


[*] posted on 14-5-2018 at 03:43


What you did is a a good separation method. Mg(OH)2 is insoluble, but sodium sulfate is quite soluble. Any method of removing the precipitate and keeping the solution will work. So you can either filter or decant the liquid, but please be more patient with both methods. Chemistry takes time.

[Edited on 14-5-2018 by CobaltChloride]

[Edited on 14-5-2018 by CobaltChloride]
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 14-5-2018 at 09:48


u need suction filtration if u want faster separation.



View user's profile View All Posts By User
RogueRose
International Hazard
*****




Posts: 1597
Registered: 16-6-2014
Member Is Offline


[*] posted on 14-5-2018 at 21:08


Mg(OH)2 is a major PITA to filter and even allowing to seperate. I'd find a large vessel and add a lot of water which will dilute the Na2SO4 as much as possible. Allow to settle and decant. Repeat as many times as you see fit.

Time is your best ally in this endeavor and while it may seem like a PITA to wait, it provides the best results.

You don't happen to have a centrifuge by any chance do you? I've wanted to get/make one for some time for this type of situation so the precipitate will just stick to the wall and the liquid will flow out. It seems a better solution when working with difficult precipitates such as this and others like CaSO4.
View user's profile View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 18-5-2018 at 14:51


My experience is that freezing (or near freezing) a solution with a fine suspension, and then allowing to warm, appears to assist in the settlement process.

Another path, best with a well sealed plastic vessel containing the suspension, is to employ a centrifuge or a home version (like a spin only setting on the washing machine).
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2802
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 18-5-2018 at 15:00


You might want to look up Sorel cements. MgO and MgSO4 form an insoluble double salt. Separation is likely to be very hard.



Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Melgar
Anti-Spam Agent
*****




Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline

Mood: Estrified

[*] posted on 20-5-2018 at 19:35


You might actually consider using a centrifuge if it's annoying enough. I have a friend who build his own centrifuge, and he actually uses it all the time.



The first step in the process of learning something is admitting that you don't know it already.

I'm givin' the spam shields max power at full warp, but they just dinna have the power! We're gonna have to evacuate to new forum software!
View user's profile View All Posts By User
soma
Hazard to Others
***




Posts: 297
Registered: 31-7-2010
Member Is Offline

Mood: No Mood

[*] posted on 23-5-2018 at 03:24


Any information on how to build a centrifuge? I'd be interested.
View user's profile View All Posts By User
LearnedAmateur
National Hazard
****




Posts: 513
Registered: 30-3-2017
Location: Somewhere in the UK
Member Is Offline

Mood: Free Radical

[*] posted on 23-5-2018 at 06:11


I’ve always thought an easy to make one would be from an old bike, change the pedals to handles or use as is, and high torque is converted to a fast spin with large gears with the sample secured to the edge of the wheel and with bits removed so it doesn’t hit the frame. Alternately, there’s this if you want to prep something on the micro-micro scale for less than a dollar/pound/[insert currency here]:

https://www.nature.com/articles/s41551-016-0009

[Edited on 23-5-2018 by LearnedAmateur]




In chemistry, sometimes the solution is the problem.