Source of anhydrous aluminum chloride
So i was reading the compounds in the antiperspirant spray called old spice and it has 40 percent aluminum chloride desolved in a polar solvent butane
I was thinking of making aluminum powder
By reacting lithium with the solution i was going to use magnesium but it is not as reactive
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Aluminum chloride is not dissolved in butane (a non=polar solvent) in Old Spice.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1477
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
A quick search seems to show aluminum chloride, aluminum chlorohydrate, aluminum sesquichlorohydrate and some Aluminium zirconium tetrachlorohydrex
gly in deoderants and over the counter deoderants actually... But I saw nothin about dissolved in butane.
I found this odd, as that notion seemed highly unlikely to me at first also. Weird.
------addition-------
Recently looked into some pool chems that can be pricy locally.
One of the flock agents, HTH brand "super green to blue" pool treatment has polyaluminum chloride or aluminum polychloride( saw both while searching).
I know it works better than some other brands available here, but because half the price is a few pounds of chlorine it's not affordable. So you
could see why it might seem odd various similar agents in deoderant. The aluminum chlorohydrate came up in flocc searches several times.
[Edited on 23-4-2018 by violet sin]
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Doesn't butane merely act as a propellant in this situation?
And if you hadn't told me, I would have assumed the active ingredient to be a hydroxide of aluminium.
|
|
Amos
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline
Mood: No
|
|
Hydrated aluminium chloride is a common antiperspirant. Butane is the propellant. The actual solvent as I understand it is a mixture of water and
denatured alcohol, so if you want a great big fireball in your lab, go ahead and add lithium to it.
|
|
symboom
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline
Mood: Doing science while it is still legal since 2010
|
|
Already tried it no fire ball the white aluminum chloride just sat on top of it. Also there is no water or alcohol and another poster is right butane
is just a propellant i dont think it is desolved in it. By the way i just used the lithium from button cell batteries much easier to open and i only
need a small amount.
Aluminum chloride
Although it is soluble in hydrogen chloride, ethanol, chloroform, carbon tetrachloride none of these can be used with lithium
Not sure if benzene reacts with lithium
slightly soluble in benzene
|
|
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
If you want anhydrous aluminum trichloride, I just ordered a kilogram of it, which is a great deal more than I ever plan to use. It hasn't arrived
yet, but the order has been processed.
The first step in the process of learning something is admitting that you don't know it already.