Questions on:Colloidal Gold
Can anyone knowledgable on Gold Colloids tell me if KCN will dissolve the Gold Colloid particle? If so, please tell me how to make it soluble in KCN
or NaCN?
Respectfully,
PM
|
|
DavidJR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
KCN solution dissolves gold in general, so yes, I'd expect it to dissolve colloidal gold pretty quickly.
|
|
maddman3150
Harmless
Posts: 2
Registered: 15-1-2017
Member Is Offline
Mood: No Mood
|
|
DavidJR, Thank You, I'll give it a try.