The fiberglass or ceramic material used to make heating mantels - what is it?
There is another thread about someone trying to make a mantle and it's impossible to post pics in it or edit it for some reason, so I came hear with
the question (I know many others have the same question as well) Bascially I am trying to figure out what is the material that seperates the nichrome
(Por whatever) and the glass. I've seen some DIY's use fiberglass weave add they report that it doesn't hold up and it radiates heat and even melts
in hot spots. SO something else must be used because there are professional setups that don't look like the woven fiberglass that can handle much
higher temps I wonder what it is.
This is just chopped fiberglass mat
Attachment: f.jpgiberglass matt woven (450kB) This file has been downloaded 742 times
Woven fiberglass matt - good for repairs where strength is important. It is difficult to make a semi-circular bowl with this.
This is the material that is between the heating element and the outer steel shell to reduce the heat being output to the outside of the mantle
This is a good look for the heating mantle "fabric". The question I have is whether this is roap coiled around many times, starting at the center
bottom and working up or what? Also is the NiChrome interlaced inside the rope or fabric? What is this stuff called and what is the composition?
More pics like above - same questions. Also, can this fiber be purchased like this for this purpose or is it only custome made?
Nice side view of a basket made of the strange weave pattern. any ideas on the name of the weave pattern?
Just another view point.
![mantle - fiber basket - 500ML-250W-Fiber-White-Adjustable-Temperature-Electric-Sets-_57.jpg - 96kB](https://www.sciencemadness.org/whisper/files.php?pid=512482&aid=66706)
I'm wondering if carbon fiber could be used. It looked like Carbon fiber had a high enough heating mel;ting point to keep it from liquifying unless
melting lost 1f
[Edited on 3-30-2018 by RogueRose]
[Edited on 3-30-2018 by RogueRose]
[Edited on 3-30-2018 by RogueRose]
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1313
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Carbon fiber is electrically conductive, so you can't use it around a nichrome element.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Could be kaowool, asbestos, rock fibers, any number of ceramic textiles, really.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
nux vomica
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 267
Registered: 18-7-2013
Member Is Offline
Mood: No Mood
|
|
I wouldn't bother making your own elements I tried that idea and wasted time and materials just buy a replacement element of eBay and start from that
, I posted a thread a while ago about using a coffee can for a homemade heating mantle.
https://www.sciencemadness.org/whisper/viewthread.php?tid=67866#pid459269
|
|
yobbo II
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 728
Registered: 28-3-2016
Member Is Offline
Mood: No Mood
|
|
Stove rope
https://www.ebay.co.uk/itm/STOVE-ROPE-DOOR-SEAL-LOG-WOODBURN...
|
|