Procedure for refining brass?
I would like to be able to take scrap brass and refine it into it's constituent metals. I would then take these metals and alloy them in specific
quantities so I have a known alloy to use in metalworking projects.
It looks like electrolysis in a copper sulfate bath is the typical way to get the copper from brass, but it makes a zinc solution that needs to be
dealt with. Also, what about the other metals like lead? I've read that lead interferes with the electrolysis significantly. It would be best if
the zinc saturated copper sulfate solution could be recycled.
Or could this all be done with acids, dissolving the metals and precipitating them out with various reactions? If some chem wiz could lay out a
procedure that would be awesome, or even just cite a good source where I could learn how to do this. Thanks!
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
Wet chemistry CAN separate Cu alloys into constituent metals, but it does not pay to do so industrially.
Generally, when going to recycling/scrapping/metal salvage, brass is not refined to the individual elements constituting it. That would not usually be
economical. Instead, recycled brass is smelted into a batch of ingots of uniform makeup, tested and then used to make up whatever Cu alloys are
desirable and make economic sense from a particular batch.
Any large ammounts of alloying materials tend to make electrolytic Cu refining go poorly.
You CAN boil most of the Zinc out of smelted brass, capture the ZnO and use it to make up a different alloy, or reduce it to pure Zn. In fact, most
brass foundries do their best to capture Zn escaping a melt, often adding it to a subsequent batch of brass.
What is your target alloy? Which brasses do you have for raw material.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
Anjali
Harmless
Posts: 1
Registered: 15-3-2018
Location: Kota
Member Is Offline
Mood: No Mood
|
|
he main component of brass is copper. The amount of copper varies between 55% and 95% by weight depending on the type of brass and its intended use.
Brasses containing a high percentage of copper are made from electrically refined copper that is at least 99.3% pure to minimize the amount of other
materials. Brasses containing a lower percentage of copper can also be made from electrically refined copper, but are more commonly made from
less-expensive recycled copper alloy scrap. When recycled scrap is used, the percentages of copper and other materials in the scrap must be known so
that the manufacturer can adjust the amounts of materials to be added in order to achieve the desired brass composition.
The second component of brass is zinc. The amount of zinc varies between 5% and 40% by weight depending on the type of brass.
A diagram depiding typical manufacturing steps in 6rass production.
A diagram depiding typical manufacturing steps in 6rass production.
Brasses with a higher percentages of zinc are stronger and harder, but they are also more difficult to form and have less corrosion resistance. The
zinc used to make brass is a commercial grade sometimes known as spelter.
Some brasses also contain small percentages of other materials to improve certain characteristics. Up to 3.8% by weight of lead may be added to
improve machinability. The addition of tin improves corrosion resistance. Iron makes the brass harder and makes the internal grain structure smaller
so that the metal can be shaped by repeated impacts in a process called forging. Arsenic and antimony are sometimes added to brasses that contain more
than 20% zinc in order to inhibit corrosion. Other materials that may be used in very small amounts are manganese, silicon, and phosphorus
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1702
Registered: 24-9-2005
Member Is Online
Mood: Bored
|
|
Honestly it's a terrible idea, refining any real amount of metal will take a LOT of time and energy. If you simply want to make your own alloy you're
much better of starting with copper scrap and zinc.
We're not banging rocks together here. We know how to put a man back together.
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Or as Bert said, melt it all together and test it to figure out the overall composition. Then you can add in extra copper or zinc to get you to your