help with drying out ammonium nitrate please
i have obtained some ammonium nitrate but it's contains alot of moisture, what is a good method to dry it out could i use magnesium sulfate which
has been dryed in an oven and what temperature should be used. Is it fairly safe to dry with a gas burner
|
|
Microtek
National Hazard
  
Posts: 921
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
Dry it in the oven at 120 C. This drives out enough of the moisture for most purposes.
|
|
Haggis
Hazard to Others
 
Posts: 238
Registered: 1-12-2002
Location: Mid-America.
Member Is Offline
Mood: Lacrymating
|
|
Yes, heating will be the best bet. Like Microtek said, 120 is a good round about temperature. Dessicating will only take a long time and more
effort. You can do this either by spreading it out on a baking pan in the oven or a small amount in beaker heating while you stir it constantly. For
some reason I think that you got your ammonium nitrate from a coldpack that has already been used, am I right?
|
|
vulture
Forum Gatekeeper
   
Posts: 3330
Registered: 25-5-2002
Location: France
Member Is Offline
Mood: No Mood
|
|
The problem with dessicating is that ammoniumnitrate itself is an extremely good dessicant, far superior to magnesiumsulfate.
One shouldn't accept or resort to the mutilation of science to appease the mentally impaired.
|
|
Christopher
Harmless
Posts: 4
Registered: 22-11-2002
Location: australia
Member Is Offline
Mood: No Mood
|
|
I did get it from an intant cold packs, i hadn't used them, but for some reason the prilled ammmonium nitrate looked and felt a bit wet .Which I
though was a little weird. It's possible moisture could have got into the bag which was quite thin or the liquid isn't water at all. The
ammonium nitrate might have be treated so it's not suitable for other purposes. I haven't done anything thing with it yet, because
i want research the chemical for safety and it's uses.
thanks for your advice it's a great help
|
|
Darkfire
Hazard to Others
 
Posts: 292
Registered: 3-1-2003
Location: California
Member Is Offline
Mood: Wondering
|
|
It likley wet because the goverment wants to stop people from using is as explosives...thats my guess at least...
\"I love being alive and will be the best man I possibly can. I will take love wherever I find it and offer it to everyone who will take it. I
will seek knowledge from those wiser and teach those who wish to learn from me.\" Duane Allman
|
|
DDTea
National Hazard
  
Posts: 940
Registered: 25-2-2003
Location: Freedomland
Member Is Offline
Mood: Degenerate
|
|
I think the government would find better ways to stop people from using AN as an explosive... after all, can't wet AN still be used to make ANNM
and APAN? If I recall correctly, only ANFO does not work properly with wet AN.
|
|
Christopher
Harmless
Posts: 4
Registered: 22-11-2002
Location: australia
Member Is Offline
Mood: No Mood
|
|
This is going to sound a little goofy but I looked at the ammonium nitrate and it's seems pretty dry and i haven't done anything to it and
it was in a well sealed container. I guest i didn't eximine it close enough , the prills were shine though, I didn't touch the chemical
much, because it not the healthest thing to do.
I did some research and found that prilled ammonium nitrate is usually coated with a conditioning agent for ease of handling and storage. A substance
used for this is
kieselguhr there could be others if you know any please tell
|
|
Marvin
National Hazard
  
Posts: 995
Registered: 13-10-2002
Member Is Offline
Mood: No Mood
|
|
I think I have to disagree vulture. AN is not very powerful dessicating agent at all in my experience. Anhydrous magnesium sulphate on the other
hand is a pretty damn good one, both in terms of ultimate H2O concentration, and total absorbed.
My AN assuming no water of crystalisation, is quite stable and dry inside the house unsealed and seems roughly comparable to sodium nitrate.
|
|
a123x
Hazard to Self

Posts: 87
Registered: 12-1-2003
Member Is Offline
Mood: No Mood
|
|
I too have gotten coldpacks that have the AN moistened. I just dry it out in small amounts whn I need tous it with a small coffee mug warmer. It only
gets to like 60-70C at the most I think but I live i a decently dry area so it works. The coffee mug warmer even will dehydrate copper sulfate
hexahydrate. I'm a bit annoyed because it seems some KNO3 I got is moistened a bit but it isn't as if I can't dry that out either.
|
|
CHEMxpl
Harmless
Posts: 21
Registered: 14-11-2016
Member Is Offline
Mood: No Mood
|
|
i just finished drying a batch of ammonium nitrate in an oven at 160C and one big mistake i made was using a 416 stainless steel plate.
and it reacted a bit with it so use some other grade or metal.
it's very easy
|
|
Chlorine
Hazard to Self

Posts: 56
Registered: 26-11-2016
Location: Maine, USA
Member Is Offline
Mood: Brominated
|
|
You should recrystallize before you dry it, most instant cold packs contain an anti-caking agent on the ammonium nitrate pellets. Then you should dry
in an oven around 120-130 C.
|
|
Texium
|
Thread Moved 26-11-2016 at 09:37 |
Dwarvensilver
Hazard to Self

Posts: 52
Registered: 8-6-2016
Member Is Offline
Mood: Constantly Chemically Amazed
|
|
Agreed, Recrystalization of suspect chemicals is a really great way to clean them up, I had ~20kg of lead nitrate that was poorly opened and used and
I think got copper sulfate in it as it had a blue tinge to it even when 100g was dissolved in DDI H20 but the crystallized material from it was snow
white.
There is nothing more useless than doing well that which need not be done at all.
|
|
ecos
Hazard to Others
 
Posts: 464
Registered: 6-3-2014
Member Is Offline
Mood: Learning !
|
|
easy thing is to put it in a box and make a hot lamp very close to it.
|
|
Fulmen
International Hazard
   
Posts: 1752
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
The solubility of ammonium nitrate increases greatly with temperature. "Shock heating" can cause it to melt. The ideal approach would be forced air,
ramped in several steps up to 120°C.
[Edited on 27-11-16 by Fulmen]
We're not banging rocks together here. We know how to put a man back together.
|
|
midlifer
Harmless
Posts: 2
Registered: 22-12-2017
Member Is Offline
Mood: No Mood
|
|
AN from cold packs or fertilizer
I've taken AN from fertilizer and cold packs and dissolved it in distilled water and, after filtering it, used a hot air cooker to dry it. I've also
used a small slow cooker. Both worked well (though I'm not sure that all the water of crystallization was removed).
I've also heated the solution in a large beaker to about 170 degrees C on a lab hotplate. (May not be the safest way, but I watch it carefully,
monitoring the temp.) Be careful because the stuff will turn hard as concrete when it cools. I also think one batch reached the AN boiling point of
about 210 degrees C: it stopped boiling like water and the liquid AN started to make a popping sound with each bubble and releasing nitrous oxide. (I
think.)
The most tedious way, but for my needs, the best way is to avoid water in the first place. I dissolve in methanol, filter, cover the beaker with
plastic wrap secured by a large rubber band, and place in the freezer. In about two hours you have a bunch of WATER-FREE AN precipitate. Filter, dry
and do it again.
Keep in mind that water is a MUCH better solvent, but such a pain to drive out.
That's my take on it. Any critical comments appreciated.
|
|
chloric1
International Hazard
   
Posts: 1162
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline
Mood: Stoichiometrically Balanced
|
|
Quote: Originally posted by Fulmen  | The solubility of ammonium nitrate increases greatly with temperature. "Shock heating" can cause it to melt. The ideal approach would be forced air,
ramped in several steps up to 120°C.
[Edited on 27-11-16 by Fulmen] |
This might be what I’m dealing with “shock heating” as I had the ammonium nitrate at only 120 Celsius but it melted. That’s a full 40+ less
than the designated melting point of ammonium nitrate. It is solid at room temperature
Fellow molecular manipulator
|
|
Sir_Gawain
Hazard to Others
 
Posts: 497
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline
Mood: Still in 2022
|
|
You have to start at a low temperature (~80°C) and slowly increase over time. Stir frequently or it will fuse into a solid brick.
[Edited on 9-11-2024 by Sir_Gawain]
“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
|
|
chloric1
International Hazard
   
Posts: 1162
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline
Mood: Stoichiometrically Balanced
|
|
Yeah I got the crazy ammonium nitrate into a cake and warmed it slightly so I could remove it from my crystallization dish. I don’t care how many
inorganic synthetic preparations you read, there are mechanical aspects of chemistry you have to work out yourself. This forum is fantastic for
pooling collective hands on experience though!
Fellow molecular manipulator
|
|
Chemgineer
Hazard to Others
 
Posts: 225
Registered: 25-5-2021
Member Is Offline
|
|
I got a cheap food dehydrator from Amazon and that dries out ammonium nitrate quite nicely over several hours. It's basically a mild heater (around
70 degrees) and a fan.
[Edited on 12-9-2024 by Chemgineer]
|
|
ManyInterests
National Hazard
  
Posts: 969
Registered: 19-5-2019
Member Is Offline
|
|
Quote: Originally posted by Chemgineer  | I got a cheap food dehydrator from Amazon and that dries out ammonium nitrate quite nicely over several hours. It's basically a mild heater (around
70 degrees) and a fan.
[Edited on 12-9-2024 by Chemgineer] |
Sometimes improvised lab gear is the best!
|
|
Precipitates
Hazard to Others
 
Posts: 161
Registered: 4-12-2023
Location: SE Asia
Member Is Offline
Mood: Acid hungry
|
|
When I produced AN about 10 years ago I dried from methanol in direct sunlight.
Did take a couple of weeks of sunny days to completely dry though (otherwise known as a long UK summer!).
|
|
Random
International Hazard
   
Posts: 1120
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
I had a solution of it. It actually dried during winter.
In Summer it caught Moisture.
|
|