Fusionfire
Hazard to Others
 
Posts: 219
Registered: 8-7-2011
Member Is Offline
Mood: No Mood
|
|
DIY high temp. superconductors
Both of these superconductors work at temperatures above the BP of liquid nitrogen.
http://en.wikipedia.org/wiki/YBCO
http://en.wikipedia.org/wiki/BSCCO
Has anyone been able to make them as an amateur chemist at home? How did you do it and what were the results?
|
|
phlogiston
International Hazard
   
Posts: 1381
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
No idea, but this looks like a nice, spectacular synthesis:
http://www.youtube.com/watch?v=-JLWeYQFA2I
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
Fusionfire
Hazard to Others
 
Posts: 219
Registered: 8-7-2011
Member Is Offline
Mood: No Mood
|
|
Very nice. When I come back from holidays I'd like to try that
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
What were the reactants? The video doesn't say, but if I had to guess it would be barium carbonate, yttrium oxide and copper oxide.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Steam
Hazard to Others
 
Posts: 238
Registered: 25-3-2014
Location: Minnesota
Member Is Offline
Mood: Triple Point
|
|
YBCO can be made by heating the metal carbonates at temperatures between 726.85- 1030 C
4BaCO3 + Y2(CO3)3 + 6CuCO3 + Excess O2 --> 2YBa2Cu3O7 + 13CO2
Suppose this could be done in a furnace
Otherwise I found this article using the metal oxides to make YBCO
http://scitech.au.dk/fileadmin/site_files/formidling/Superle...
[Edited on 26-3-2014 by Steam]
DISCLAIMER: The information in this post is provided for general informational purposes only and may not reflect the current law in your jurisdiction.
No information contained in this post should be construed as legal advice from the individual author, nor is it intended to be a substitute for legal
counsel on any subject matter. No reader of this post should act or refrain from acting on the basis of any information included in, or accessible
through, this post without seeking the appropriate legal or other professional advice on the particular facts and circumstances at issue from a lawyer
licensed in the recipient’s state, country or other appropriate licensing jurisdiction.
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Can't say I enjoy that method, as I have no pressure devices or high-temperature devices.
Where, then, would be a cheap place to buy YBCO disks?
Cheapest I've seen was $50 per disk, here: http://shop.can-superconductors.com/demonstration-kits/13-dk...
Also found this, but I get the strangest feeling they're selling me the powder, and I don't think I can sinter it without removing the properties: http://www.americanelements.com/ybacuo.html
Also, don't know the price for that last one.
How do universities get their hands on these materials? They can't seriously all be manufacturing their own, that's pre-Industrial Revolution style
thinking.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
LabGuy
Harmless
Posts: 1
Registered: 11-1-2018
Member Is Offline
Mood: No Mood
|
|
this is how YBCO can be made: https://www.youtube.com/watch?v=XjuUMVm3hZ8
2 step process gives much better results: https://www.youtube.com/watch?v=FBDWn1ltZDI
|
|