jpsmith123
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 764
Registered: 24-6-2005
Member Is Offline
Mood: No Mood
|
|
Hydrazine Sulfate As A reducing Agent For Electroless Plating
Does anyone know if hydrazine sulfate can replace the sodium hypophosphite or borohydride used as a reducing agent in electroless plating? Apparently
its use in this manner is mentioned in some patents, but there's not a lot of practical information on it.
Regards,
Joe
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Online
Mood: No Mood
|
|
well, this site
http://66.102.9.104/search?q=cache:pMhyPEJzZr8J:boyles.sdsmt.edu/cumirror/cumirr.ppt+%22copper+mirror%22+hydrazine&hl=en
says you can plate copper using hydrazine as a reductant.
|
|
jpsmith123
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 764
Registered: 24-6-2005
Member Is Offline
Mood: No Mood
|
|
Thanks for the interesting link.
Based on the little tidbits of information I've seen, it seems that hydrazine sulfate may also work.
Just in case it doesn't, though, I wonder what would be the best way to get a dilute aqueous hydrazine solution from the sulfate?
Regards,
Joe
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
Add a strong base, e.g. NaOH.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Online
Mood: No Mood
|
|
BTW, you do know that hydrazine is volatile and a suspect carcinogen, don't you?
|
|
jpsmith123
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 764
Registered: 24-6-2005
Member Is Offline
Mood: No Mood
|
|
In water or alcohol or some other solvent? What's the rest of the process?
The devil's in the details...what are they?
Quote: | Originally posted by neutrino
Add a strong base, e.g. NaOH. |
|
|
neutrino
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline
Mood: oscillating
|
|
Something like this should happen:
N<sub>2</sub>H<sub>6</sub>SO<sub>4</sub> + 2 NaOH ->
N<sub>2</sub>H<sub>6</sub>(OH)<sub>2</sub> + Na<sub>2</sub>SO<sub>4</sub>
N<sub>2</sub>H<sub>6</sub>(OH)<sub>2</sub> -> N<sub>2</sub>H<sub>4</sub> + 2
H<sub>2</sub>O
The spectator ions should be ignorable, although you know more about plating than I do. If they do pose a problem, see Rosco's posts in the
hydrazine thread.
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
Cold dilute aqueous solutions of hydrazine should be relatively harmless though.
If he is making up the plating solution, doing the plating and then disposing of the solution safely he should be OK.
[Edited on 15-11-2011 by ScienceSquirrel]
|
|
Jor
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 950
Registered: 21-11-2007
Member Is Offline
Mood: No Mood
|
|
I've done it by dissolving copper(II) acetate in water, add ammonia until all initially formed Cu(OH)2 dissolves, add hydrazine hydrate and heat on a
water bath.
http://amateurchemie.nl/viewtopic.php?f=20&t=404
|
|
cyanureeves
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
Jor does your method plate regular carbon steel ?or is this just for silver mirror type plating?
[Edited on 16-11-2011 by cyanureeves]
|
|
Jor
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 950
Registered: 21-11-2007
Member Is Offline
Mood: No Mood
|
|
I don't know. You should try it.
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
is there some alternative to hydrazine here?
|
|
Random
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1018
Registered: 7-5-2010
Location: In ur closet
Member Is Offline
Mood: Energetic
|
|
is there some alternative to hydrazine here?
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6269
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
I was thinking about creating a copper mirror. I have spotted a youtube video showing a method using hydrazine -- which is essentially the same as
the method above. https://www.youtube.com/watch?v=tkFOzFNODUE
However, I do not have access to hydrazine and synthesising it will be a new step for me. I could go there but wondered if alternatives to the
hydrazine exist.
|
|
JJay
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3440
Registered: 15-10-2015
Member Is Offline
|
|
Hydrazine is rather nasty - carcinogenic, explosive, low-boiling, and poisonous; I don't think playing with it in an amateur lab is a good idea.
|
|