proxymethoxy
Harmless
*




Posts: 9
Registered: 7-7-2015
Member Is Offline

Mood: No Mood

[*] posted on 6-9-2015 at 08:54
Methylamine hydrochloride reacting with copper


I synthesised a batch ot methylamine hydrochloride and after recrystalization and chloroform wash I transfered the bulk of it to a vacuum chamber with a few NaOH pellets. I used a metalic spoon to collect the last bit of methylamine from the buchner and sometime later, not having cleaned my spoon, I noticed it had gone green where wet methylamine was deposited.

Could anyone give me an idea of the reaction taking place?
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 6-9-2015 at 09:24


CH3-NH2.HCl <==--> CH3-NH2 + HCl

Cu + moist air --> superficial CuO + Cu(OH)2 + CuCO3

CuO + 2 HCl --> CuCl2 + H2O
Cu(OH)2 + 2 HCl --> CuCl2 + 2 H2O
CuCO3 + 2 HCl --> CuCl2 + CO2(g) + H2O

CuCl2 + 4 CH3-NH2 --> Cu(CH3-NH2)4Cl2 (or CuCl2.4 CH3-NH2)
Tetramethylamino copper (II) chloride complex




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 7-9-2015 at 08:18


Most lower amines attack copper.
View user's profile View All Posts By User
Rosco Bodine
Banned





Posts: 6370
Registered: 29-9-2004
Member Is Offline

Mood: analytical

[*] posted on 9-9-2015 at 23:28


IIRC Methylamine does not complex copper
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 10-9-2015 at 09:42


It may not complex but it does attack.
Other things that are known to attack copper with better documentation.

Hexamethlene diamine
Hexamine
Ammonia
Urea

I certainly can't find any references that say it resists methylamine.
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 10-9-2015 at 09:54


Quote: Originally posted by Rosco Bodine  
IIRC Methylamine does not complex copper

Why wouldn't it?
Ammonia, hydrazine (sometimes with decomposition), ethylenediamine do form complexes...methylamine is more basic than ammonia and as such its free doublet is more prone to complexate.

There are structural references for Tetrakis(methylamine)dibromocopper.

There are also references for CuCl2 methylamine and Cu(HCO2)2 methylamine complexes decomposition pressure and heat of decomposition.
methylamine complex CuCl2 and Cu(HCO2)2.jpg - 207kB




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 10-9-2015 at 10:32


Personally I think it probably does complex.
Rosco has his doubts.
View user's profile View All Posts By User
Rosco Bodine
Banned





Posts: 6370
Registered: 29-9-2004
Member Is Offline

Mood: analytical

[*] posted on 10-9-2015 at 14:46


Actually it was trimethylamine that I was thinking of does not form a complex with copper. So it could be that methylamine or dimethylamine does complex copper.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 10-9-2015 at 16:17


I would be very surprised if methylamine did not attack copper, especially in the presence of methylammonium salts.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
proxymethoxy
Harmless
*




Posts: 9
Registered: 7-7-2015
Member Is Offline

Mood: No Mood

[*] posted on 12-9-2015 at 09:02


Great input everyone, thanks! This forum seems to host some pretty smart folk ;)
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 12-9-2015 at 09:04


There are some amazingly smart and experienced people here.

There are Others as well.




View user's profile View All Posts By User
Rosco Bodine
Banned





Posts: 6370
Registered: 29-9-2004
Member Is Offline

Mood: analytical

[*] posted on 26-11-2017 at 17:17


Here is a relevant paper describing some complexes of copper and methylamine

Attachment: Substances_Formed_by_the_Interaction_of.pdf (399kB)
This file has been downloaded 314 times
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 30-11-2017 at 17:47


Ummm. Why not chloroform plus copper?

If you have residual Chloroform in you product, given a little heat (or time?), chloroform and copper might react.
View user's profile View All Posts By User
LearnedAmateur
National Hazard
****




Posts: 513
Registered: 30-3-2017
Location: Somewhere in the UK
Member Is Offline

Mood: Free Radical

[*] posted on 1-12-2017 at 09:40


But what would be the product of that reaction? I thought chloroform was fairly inert hence its usefulness as an organic solvent; it takes a bit of a budge to make copper react with most reagents that it can. Here you've got a base with an amphoteric material, so I would've thought that would be the observed reaction.

Edit: I can't find any information on whether dichlorocarbene (:CCl2, generated from CHCl3 and NaOH for those who don't know) reacts with copper metal by itself or with any other present reagent. Might be something to look into.

[Edited on 1-12-2017 by LearnedAmateur]




In chemistry, sometimes the solution is the problem.

It’s been a while, but I’m not dead! Updated 7/1/2020. Shout out to Aga, we got along well.
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2725
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 1-12-2017 at 19:05


I think NaOH will dissolve copper to make sodium cuprate, won't it? CuO is amphoteric IIRC.

[Edited on 2-12-2017 by clearly_not_atara]




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 1-12-2017 at 21:45


Quote: Originally posted by clearly_not_atara  
I think NaOH will dissolve copper to make sodium cuprate, won't it? CuO is amphoteric IIRC.

[Edited on 2-12-2017 by clearly_not_atara]
I'm pretty sure it won't attack copper metal.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 3-12-2017 at 16:10


Um. Once for a lab class, we attempted to fractionally distill a chlorinated hydrocarbon (carbon tet.?) utilizing stainless steel "scrungy" column packing. Ran short on stainless steel, and attempted to substitute a copper plated material (steel?).

At "tet" distillation temperature....instant and dramatic corrosion.
View user's profile View All Posts By User