RogueRose
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1590
Registered: 16-6-2014
Member Is Offline
|
|
Non-oxidizing or corrosive lubricant for aluminum drilling
I have a lot of Al billots and ingots, and I need Al shavings, "swarf", powder and cuttings. My drill press works well with my tungsten carbide bits
but it seems that I am going to need to add some kind of fluid to lubricate (and possibly cool) the cutting. I'm using 3/8 - .5" bits as well as
stepped sheet metal bits that starts at 3/8" and ends at 1 3/8" - with each level increasing by 1/8". These are often used for hardened steel sheet
metal and even cast iron, but they work find for Al (the ones I have do at least).
I'm wondering if there is some common fluid that I can use that will not effect the Al shavings, chips, etc. I would think water may oxidizer or cause
other problems.
I do have old cooking oil (not sure content), I also have:
Liquid soap (100% coconut oil soap about 1:10 soap to water - could be watered down to strenghened)
Dish soaps ( Dawn, Palm olive and the like)
-coconut oil
-palm oil
-olive oil
-Saffllower oil
-Sunflower oil
-castor oil
-pork lard
-Beef Tallow
-Glycerol
-Motor oil - 10w30
-household 3-in-1 oil (not much left though)
-WD40
-Regular Diesel
-Biodiesel
-E85
-55-60% ethanol (rest is water)
-little mineral oil (best used for my beat bath though...)
-Ethylene glycol (pure concentrate anti-freeze - with stabilizers and other
-Windshield washer fluid
others that may be helpful
Na2CO3
NaHCO3
Borax
urea
TriSodium Phosphate
After the cutting is done, I'll have to strain the fluid, remove the chunks/shavings/powders so I can use the fluid again if possible. I'm just not
sure how I can clean the shavings so that they don't have the oil on them or any residue, or have the Al react with any of this.
On a side note, I'm probably going to be doing the same thing with Mg slabs and probably Mg/Al slabs, but that won't be for a couple months.
Can anyone give any suggestions on which would be the best method to lubricate the drilling and not damage the Al shavings in any part of the process?
Much appreciate to anyone who can point me in a good direction for this. Thanks a lot and the best to ya'll!!
|
|
JJay
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3440
Registered: 15-10-2015
Member Is Offline
|
|
Cooling fluid isn't usually required for aluminum with a drill press, but you could probably use cutting oil (which is a fluoridated petroleum I
believe). Compressed air and water might be options also.
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1311
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
I used kerosene regularly in the machine shop.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1702
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
A good cooling liquid is quite beneficial when machining aluminium. It turns soft and "gummy" as heat builds up, this in turn will increase friction
between the tooling, workpiece and chips. Chips can easily weld itself to the tooling or workpiece if left unchecked.
I mainly use oil dispersions as I have flood cooling on the lathe. Water also removes heat more effectively. Flood (or mist) cooling is obviously the
most effective as it can remove more heat, but it also makes a mess. It's fine in a machine with a chip tray and water sump, not so nice on a drill
press on a wooden work bench.
Almost any cutting fluid should help, the standard choice in machine shops used for most machining is a appr 4% oil emulsion in water. For aluminium
straight mineral oils (like WD40 or CRC 556) are often used, some claim alcohol is the best for HSS tooling when a good finish is required. I guess it
often boils down to personal preferences and availability/convenience.
There are also special cutting fluids (extreme pressure additives) based on sulfurized oils or chlorinated hydrocarbons. I make my own by heating rape
seed oil with appr. 5% sulfur, it makes a huge difference for high-load operations like tapping and threading harder materials. But I don't think it
will be necessary for drilling aluminium.
We're not banging rocks together here. We know how to put a man back together.
|
|
RogueRose
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1590
Registered: 16-6-2014
Member Is Offline
|
|
Thanks for the replies, I noticed someone said something about "It turns soft and "gummy" as heat builds up" - I'm wondering if some type of soap
would work for this, like bar soap on the bit, or a diluted solution into the whole.
I'll just have to see how much it changes the A for the Final product. Thanks again!
|
|
bobm4360
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 59
Registered: 18-4-2011
Location: On a wretched little island.
Member Is Offline
Mood: No Mood
|
|
"A-9" from an industrial supply works with both Al and Mg, and cleans easily with methyl ethyl ketone or acetone. For cleaning chips, put 'em in a
bucket or saucepan and wash 2 or 3 times by decantation. Both metals oxidize very quickly and will have a thin (molecular layer) oxide coat as soon
as the metal is exposed to air. This layer stops further oxidation of Al; but Mg oxidizes quite a bit deeper.
[Edited on 25-10-2017 by bobm4360]
|
|
Fulmen
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1702
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
Soap could reduce friction, but so will lard or motor oil. And they would probably handle the high temperatures better. Reducing friction is only part
of the solution anyway, as the cutting inevitably produces heat. I'm not sure if soap handles heat as well as lard or regular oil will, so you could
end up with burning the soap causing more problems than it solves.
We're not banging rocks together here. We know how to put a man back together.
|
|
Bezaleel
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 444
Registered: 28-2-2009
Member Is Offline
Mood: transitional
|
|
Quote: Originally posted by RogueRose ![](images/xpblue/lastpost.gif) | Thanks for the replies, I noticed someone said something about "It turns soft and "gummy" as heat builds up" - I'm wondering if some type of soap
would work for this, like bar soap on the bit, or a diluted solution into the whole.
I'll just have to see how much it changes the A for the Final product. Thanks again! |
Apart from "A-9", as bobm4360 mentions, there exist standard drilling fluids for light metals and copper. These both enhance cutting properties (which
is what you want) and cool and lubricate. They are relatively expensive, though.
Another one that works for me is methylated spirits (just the cheap blue stuff). Obviously, if you take the cleaner white spirits (I assume this will
also work) you won't have a minor amount of residue left on evaporation. For me, this worked surprisingly well when working with HSS drills in
aluminium.
I advise you to stick to using lighter molecules, because the longer chains are more difficult to remove, rendering you aluminium unclean.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Or possible alternatives;
Melt the aluminium and pour it into water to form smaller lumps
Use the lumps as is, or use a ball mill to pulverise them.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I'd use engine oil- because I have plenty and it will do the job.
Then I'd remove it with a lighter oil- maybe WD40.
If you need to, you can remove what's left with lighter fluid (carefully).
Alcohols risk reacting.
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
If you can disclose the purpose you have for these (flammable?) metal particles, it might help.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|