platinum leaf for perchlorate cells?


https://www.goldleafsupplies.co.uk/gold-metal-leaf/platinum/

Seems a reasonable price, I was wondering if these are thick enough to use for perchlorate/chlorate cells etc?

I was thinking of covering titanium with them, not sure exactly how I would attach, but it would be a reasonable (price wise) way of using it. maybe two sheets per side??

Any thoughts on this approach?
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3631
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 18-10-2017 at 00:22


Due to a very thoghtful secret santa, I have a booklet of the transfer platinum foil from that supplier,
I also bought titanium foil and a bullion bar to cover with the platinum,
I still have the ingredients, but no recipe :(
I do not want to destroy my only platinum sample,
I'm considering using the foil as electrodes for the production of ozone from the air using silent electrical discharge
... on the to-do list ....

I have no perchlorate cell experience yet,
but I suspect that this foil is too fragile to use as an anode coating,
I hope that I'm proved wrong.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 18-10-2017 at 02:51


I thought it might be too thin, but then again if its got anode to coat, it might be ok?? I dont know how thick the coating is on a platinum anode, but it cant be much thicker than the foil.

For the price it might be worth doubling the amount, and making sure the anode itself is well covered. So many fake platinum anodes on ebays, at least this company has a very good rep.

Would be an easy solution if it works :D
View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 513
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 18-10-2017 at 09:22


Quote: Originally posted by NEMO-Chemistry  
I thought it might be too thin, but then again if its got anode to coat, it might be ok?? I dont know how thick the coating is on a platinum anode, but it cant be much thicker than the foil.

For the price it might be worth doubling the amount, and making sure the anode itself is well covered. So many fake platinum anodes on ebays, at least this company has a very good rep.

Would be an easy solution if it works :D


You still haven't said how you would make it adhere to the titanium. I'm pretty sure most size would dissolve in a perchlorate cell.
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 18-10-2017 at 18:34


Quote: Originally posted by Deathunter88  
Quote: Originally posted by NEMO-Chemistry  
I thought it might be too thin, but then again if its got anode to coat, it might be ok?? I dont know how thick the coating is on a platinum anode, but it cant be much thicker than the foil.

For the price it might be worth doubling the amount, and making sure the anode itself is well covered. So many fake platinum anodes on ebays, at least this company has a very good rep.

Would be an easy solution if it works :D


You still haven't said how you would make it adhere to the titanium. I'm pretty sure most size would dissolve in a perchlorate cell.


Does it have to be stuck? What about tightly wrapped and crimped over? Bit like foil round chewing gum.

First i got to decide if its worth trying, if the foil isnt thick enough then all else is a mute point.
View user's profile View All Posts By User
wg48
National Hazard
****




Posts: 821
Registered: 21-11-2015
Member Is Offline

Mood: No Mood

[*] posted on 18-10-2017 at 22:03


I could not find the thickness for any platinum leaf but I eventually found the thickness of some gold leaf at between 0.1um to 0.8um. So I will assume that platinum is 0.5um that’s about 32 times thinner than typical cooking aluminium foil. It will be very very weak.

Will it even survive the bubbling on an electrode? How would you crimp it? Look at a video of someone using gold leaf. It folds with a breath of air. I would think you would have to atleast glue it on with say a silver loaded epoxy. As its so thin how long will it last?
View user's profile View All Posts By User
yobbo II
National Hazard
****




Posts: 728
Registered: 28-3-2016
Member Is Offline

Mood: No Mood

[*] posted on 20-10-2017 at 13:00


https://www.amateurpyro.com/forums/topic/1629-making-potassi...

See eb666 post

Workes good.
About 50 grams perchlorate per day using one amp and chlorate as the starting material (not chLoride)
No erosion of 1 gram pt bar.
No problems at pt and ti interface.
Need to purchase one gram bar:D but will last years