How long would Urushibara catalyst (U-Ni-AA to be exact) keep its reactivity once it has been prepared? Also, how many times could a person use it
before the activity is lost and can it be recharged?
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
I have a friend who is currently doing extensive testing on Urushibara catalysts and their peformance. IIRC, you have to keep them out of contact from
oxygen (under ethanol) and they can be used multiple times if stored properly. The acid activated (with acetic acid) is the more sensitive I *think*
You might want to U2U NERV, he's doing a lot of work with these nickel catalysts and would probably offer you some good data/info and lend some
of his experience to you.
|
|
NERV
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 152
Registered: 22-9-2002
Location: USA
Member Is Offline
Mood: Fluorinated
|
|
I am currently doing work at a local collage with Urushibara Nickel catalysts. I have only done work on U-Ni-A, and U-Ni-B so far but I will tell you
my results for them as it may give you an idea for how long U-Ni-AA will last. The nickel precipitate is almost indefinitely stable at room temp, and
in full contact with the atmosphere, but as soon as you activate it with either an acid or base it needs to be kept away form the air as much as
possible as there is a slight diminishing of the catalysts potency in air (the catalyst lost almost all potency after about 2 months sitting in open
air). Also the catalyst can be used multiple times but it is not recommended as catalyst activity decreases largely with each use. The Al based
catalysts are supposedly not nearly as strong as the zinc based ones so your results may vary slightly.
hope that helps you out somewhat.
Vir sapit qui pauca loquitur.
|
|
DP
Harmless
Posts: 24
Registered: 25-7-2005
Location: AmeriKKKa
Member Is Offline
Mood: Cranky
|
|
I forgot I posted this so I never checked back... lol. Thanks for the info... this does help.
|
|