Cleaning molecular sieves?


I have some molecular sieves, some where used for drying EtOH, some drying ether and some drying DCM I was wondering if I could use these sieves for drying other reagents now that they have already been used without risk of contamination. Should I somehow wash them first then dry in oven?
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4547
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: PhD candidate!

[*] posted on 6-7-2017 at 08:35


Just drying them in the oven should be fine since you used them with volatile solvents. To test if they're dry, just take a sieve from the oven, allow it to cool in a dry place, and place it in the palm of your hand. Add a few drops of water, and it should heat up noticeably. If it doesn't, they need more time in the oven.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 6-7-2017 at 11:57


Don't put flammable solvents in the oven.
:o
It's a good idea to leave the used stuff exposed to air, outside or somewhere well ventilated for a while, then soak it with water and let it dry in air before slowly drying in an oven.