Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Molten Sodium Sulfide Electrolysis
Filippo
Harmless
*




Posts: 3
Registered: 29-4-2017
Member Is Offline

Mood: No Mood

[*] posted on 29-4-2017 at 03:56
Molten Sodium Sulfide Electrolysis


Could it be possible to obtain metallic sodium via Molten Sodium Sulfide Electrolysis?
Is it less dangerous than Molten NaOH electrolysis?
What is the procedure?
I chose Sodium Sulfide because its melting point is very low (50 Celsius degrees).
I'm trying to get every important element to build up a collection but i'd prefer to sythesize Na since it is very expensive while its salts are very cheap.
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 29-4-2017 at 04:03


https://en.wikipedia.org/wiki/Sodium_sulfide

Look in the "Properties" table. The anhydrous melting point is the relevant one.




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Filippo
Harmless
*




Posts: 3
Registered: 29-4-2017
Member Is Offline

Mood: No Mood

[*] posted on 29-4-2017 at 04:17


Whoops,in the italian wikipedia page it is reported it wa the anhydrous melting point.
https://it.wikipedia.org/wiki/Solfuro_di_sodio

Sooo,is there another sodium salt which electrolysis isn't dangerous and with a low melting point?
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6250
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 29-4-2017 at 05:01


This arrived on YT ten minutes ago.
I think it might be what you want.
https://www.youtube.com/watch?v=jCrFFVVcPUI
View user's profile View All Posts By User
Filippo
Harmless
*




Posts: 3
Registered: 29-4-2017
Member Is Offline

Mood: No Mood

[*] posted on 29-4-2017 at 05:43


Thank you,i'll do that as soon as i'll get a distillation apparatus for my birthday
View user's profile View All Posts By User
Jstuyfzand
Hazard to Others
***




Posts: 166
Registered: 16-1-2016
Location: Netherlands
Member Is Offline

Mood: Learning, Sorta.

[*] posted on 29-4-2017 at 07:29


That video by Nurdrage is phenomenal, although a proper castner cell is still cheaper in the long run I think.
View user's profile View All Posts By User
Harristotle
Hazard to Others
***




Posts: 138
Registered: 30-10-2011
Location: Tinkerville
Member Is Offline

Mood: I tink therefore I am

[*] posted on 30-4-2017 at 04:31


It occurs to me that the standard enthalpy of formation for aluminium oxide is even higher at -1675 kj/mol. (compared to sodium oxides -416 kj/mol). This suggests that aluminium turnings would be even better*. I guess there is the old stable aluminium oxide problem, but the same is true for magnesium.

Any reason it wouldn't work with Al powder/ turnings?

* yeah ok, kinetics isn't thermodynamics.

[Edited on 30-4-2017 by Harristotle]
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6250
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 30-4-2017 at 05:19


Standard enthalpy of formation in kJ/mol:
MgO: −601.6
Al2O3: −1669.8
NaOH: −425.9


So,
2Mg + 2NaOH = 2Na + 2MgO + H2, ΔH = -175.7 per mole of Na
2Al + 3NaOH = 3Na + Al2O3 + 1½H2 ΔH = -130.7 per mole of Na

So as a first approximation (excluding temperature calculations), Mg is more energetically favourable than Al.

I thought of the same thing myself. And since Al is so much easier to obtain that Mg, I think it is worth a try. Quite what effect this will have on the work up, I am not sure. If aluminium works then it brings sodium well into the realm of an OTC synthesis. And that is a game changer.
View user's profile View All Posts By User

  Go To Top