Harlan
Harmless
*




Posts: 4
Registered: 23-4-2017
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2017 at 13:02
Melting sodium metal into solid blob


I'm trying to melt sodium metal for a project. What I've tried so far is melting it in a pyrex based double boiler (mineral oil in both) and I worked well for melting the sodium. The problem is the sodium formed little balls instead of a single mass. I think it's the oxide layer preventing the individual balls from coalescing.

Is there an easy solution? I did see someone use isopropyl I think to dissolve the surface layer and get it into a single mass, but I haven't tried that method yet, and I only have 90% on hand.

Oh and the goal of the project is to make a sodium spoon sorta like a gallium spoon and use it in the same classic manor.
View user's profile View All Posts By User
PirateDocBrown
National Hazard
****




Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2017 at 13:20


IPA is the classic way.
View user's profile View All Posts By User
Harlan
Harmless
*




Posts: 4
Registered: 23-4-2017
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2017 at 14:00


Thanks! Any suggestions for tinning sodium to copper wire? (Separate project)
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6320
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 23-4-2017 at 14:46


I would be extremely hesitant to make a sodium spoon. That would be foolhardy.

It is likely to corrode in air which would reduce its effectiveness as a prank. But more importantly, if someone was to drop it in a hot cup of tea the resulting explosion could have dire consequences.
View user's profile View All Posts By User
Harlan
Harmless
*




Posts: 4
Registered: 23-4-2017
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2017 at 17:30


It's not intended as a prank, just a demonstration. I have a YouTube channel where I do various projects and it seemed like something different/interesting to do. I plan on releasing the spoon remotely.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1694
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 24-4-2017 at 07:18


I wonder if you could mold a spiky sodium shape with a lot of surface area or just a large flat/thin pancake, if it would go bang on the surface of the water more energetically?
View user's profile View All Posts By User
Harlan
Harmless
*




Posts: 4
Registered: 23-4-2017
Member Is Offline

Mood: No Mood

[*] posted on 24-4-2017 at 12:48


Considering the fact that it's a coulomb explosion the easier it is to get blanketed by hydrogen and electrically insulate itself the more likely it is to explode
http://cen.acs.org/articles/93/web/2015/01/Sodium-Potassium-...

[Edited on 24-4-2017 by Harlan]

[Edited on 24-4-2017 by Harlan]
View user's profile View All Posts By User
PirateDocBrown
National Hazard
****




Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline

Mood: No Mood

[*] posted on 24-4-2017 at 14:39


There's a video out there of a guy skipping a disc of sodium on water, like a skimming stone. Google it, it's quite a show.
View user's profile View All Posts By User