I'm trying to melt sodium metal for a project. What I've tried so far is melting it in a pyrex based double boiler (mineral oil in both) and I worked
well for melting the sodium. The problem is the sodium formed little balls instead of a single mass. I think it's the oxide layer preventing the
individual balls from coalescing.
Is there an easy solution? I did see someone use isopropyl I think to dissolve the surface layer and get it into a single mass, but I haven't tried
that method yet, and I only have 90% on hand.
Oh and the goal of the project is to make a sodium spoon sorta like a gallium spoon and use it in the same classic manor.
|
|
PirateDocBrown
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline
Mood: No Mood
|
|
IPA is the classic way.
|
|
Harlan
Harmless
Posts: 4
Registered: 23-4-2017
Member Is Offline
Mood: No Mood
|
|
Thanks! Any suggestions for tinning sodium to copper wire? (Separate project)
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6257
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
I would be extremely hesitant to make a sodium spoon. That would be foolhardy.
It is likely to corrode in air which would reduce its effectiveness as a prank. But more importantly, if someone was to drop it in a hot cup of tea
the resulting explosion could have dire consequences.
|
|
Harlan
Harmless
Posts: 4
Registered: 23-4-2017
Member Is Offline
Mood: No Mood
|
|
It's not intended as a prank, just a demonstration. I have a YouTube channel where I do various projects and it seemed like something
different/interesting to do. I plan on releasing the spoon remotely.
|
|
Morgan
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1675
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
I wonder if you could mold a spiky sodium shape with a lot of surface area or just a large flat/thin pancake, if it would go bang on the surface of
the water more energetically?
|
|
Harlan
Harmless
Posts: 4
Registered: 23-4-2017
Member Is Offline
Mood: No Mood
|
|
Considering the fact that it's a coulomb explosion the easier it is to get blanketed by hydrogen and electrically insulate itself the more likely it
is to explode
http://cen.acs.org/articles/93/web/2015/01/Sodium-Potassium-...
[Edited on 24-4-2017 by Harlan]
[Edited on 24-4-2017 by Harlan]
|
|
PirateDocBrown
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline
Mood: No Mood
|
|
There's a video out there of a guy skipping a disc of sodium on water, like a skimming stone. Google it, it's quite a show.
|
|