Author: Subject: Restoring Oxidised FeSO4
condennnsa
Hazard to Others
***




Posts: 217
Registered: 20-4-2010
Location: Romania
Member Is Offline

Mood: No Mood

[*] posted on 10-4-2017 at 05:50
Restoring Oxidised FeSO4


So I kept most of my chemicals after moving untouched for about 5 years now, and discovered my iron sulfate turned to this gunk:

20170410_164307.jpg - 3MB 20170410_164313.jpg - 2.9MB

The FeSO4 was prepared from battery electrolyte sulfuric acid and nails.

Honestly, I didn't know that it is not stable in air
from wikipedia: Upon exposure to air, it oxidizes to form a corrosive brown-yellow coating of "basic ferric sulfate", which is an adduct of iron(III) oxide and iron(III) sulfate:

12 FeSO4 + 3 O2 → 4 Fe2(SO4)3 + 2 Fe2O3

my question is what should I do to turn it back to pure ferrous sulfate?
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 10-4-2017 at 06:35


Recrystallize in a slightly acid solution, maybe?



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4621
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: PhD candidate!

[*] posted on 10-4-2017 at 07:26


Dissolve it in water (it will be cloudy) and then add sulfuric acid dropwise until the solution goes clear. Add a generous excess iron to the solution, and allow the iron to react until the yellow color has disappeared. Stir it well to make sure all of the solution is reduced. Then just filter off the excess iron and recrystallize it. Make sure that it's completely dry when you store it, as water will accelerate the oxidation a lot. Store it in an airtight container, densely packed together to try and exclude as much air as possible.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
Texium
Administrator
Thread Moved
10-4-2017 at 07:26

  Go To Top