Vitrifying AlNiCo magnets w/ K-glass


This is mainly in view of some tosspot having pinched my stirbars.

But I do have some AlNiCo magnets, which I read are some of the most highly coercive permanent magnets going commonly.

Anybody happen to know the vitrification temperature of a saturated soln. of potash glass? wondering if I can get away with spraying potassium silicate solution onto such a magnet and torching it in order to form a vitrified outer layer in order to protect the magnet itself from highly acidic or alkaline environments.
View user's profile View All Posts By User
Microtek
National Hazard
****




Posts: 839
Registered: 23-9-2002
Member Is Offline

Mood: No Mood

[*] posted on 12-2-2017 at 14:40


You could also put it into a glass tube of appropriate diameter, and then melt it closed.