[*] posted on 5-12-2016 at 20:21
Unknown Rock????


Workers today found the rock?? as shown in the attached photos on the side of the road.

It is a dark blue green colour with an amber sheen..
It is fibrous in nature with one end appearing denser than the other. It is quite porous.

Any ideas as to what this may be???

20161206_142450.jpg - 530kB 20161206_142524.jpg - 672kB 20161206_142620.jpg - 604kB 20161206_142647.jpg - 827kB
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1477
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline

Mood: Good

[*] posted on 5-12-2016 at 20:34


Looks just like a sample of silicon carbide I bought on saturday.

1480998533376.jpg - 866kB

Does it scratch glass like mine? I should add, the guy whom sold me that bit had several others that were similar but finer, thicker, more open and almost closed up varietys. Grabbed a small well crystalized bit of the litter.

He always hooks me up with random rocks so as to spread the wealth, and I almost never leave having spent less than $5. A small price to pay for some of the deals received over the years. If memory serves, one time he mentioned the material was man made.

[Edited on 6-12-2016 by violet sin]




View user's profile View All Posts By User
diddi
National Hazard
****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 6-12-2016 at 03:21


it looks like a micacious schist to me?

yes silicon carbide is man made. it often appears on ebay from chinese sellers as "natural" silicon stone or some such name. but it is entirely unnatural

[Edited on 6-12-2016 by diddi]




Beginning construction of periodic table display
View user's profile View All Posts By User
crystal grower
Hazard to Others
***




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 6-12-2016 at 08:42


I regognised it as SiC at the first sight too. To confirm it, test if it can scratch the glass as Violent sin said.
Im quite curious about origins of this piece, because silicon carbide is produced by reaction of Si/SiO2 with carbon at temp. Cca 1800-1900C if memory serves me well. Naturally it occurs as mineral moissanite, which was found only in meteorites.




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
sunchoau
Harmless
*




Posts: 2
Registered: 5-12-2016
Member Is Offline

Mood: No Mood

[*] posted on 6-12-2016 at 14:36


Many Thanks for the replies.

The "rock" does indeed scratch glass...in fact it is a very good glass cutter....

The general feel, from the discussion, is that is man made silicon carbide.

This piece is around 130mm long and around 60 x60 mm wide and deep.
It bears no impact marks and must have been cool or cold when deposited to where it was found....

How it got there is a mystery, however, I believe, its identity is solved.

Again,
Many Thanks for the replies.
View user's profile View All Posts By User
Eddygp
National Hazard
****




Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline

Mood: Organometallic

[*] posted on 7-12-2016 at 05:36


The fact that it scratches glass does not tell us what it is immediately, especially since SiC is man-made.
Otherwise, with the same arguments you could be holding a huge lump of black diamond or sapphire.




there may be bugs in gfind

[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
View user's profile View All Posts By User
crystal grower
Hazard to Others
***




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 7-12-2016 at 05:58


I agree that the fact it scratches glass isn't enough evidence to prove it's SiC. However, it visually looks very similiar to silicon carbide and I haven't ever seen samples of diamond, corund or other hard minerals with such habitus.

Edit: what may be a case is that it could be for example titanium carbide or some other carbide or maybe some boride.
Anyway its most likely a manmade comound IMO.
(I would be glad to find out it's a mineral though :)).


[Edited on 7-12-2016 by crystal grower]

[Edited on 7-12-2016 by crystal grower]




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 7-12-2016 at 07:49


This close up is cool. Those little clusters of what looks like quartz crystals, interspersed with the dark, ?carbide?...

Got anything else harder to test harness against, does it scatch a porcelain streak plate too? How dense...

And is there an abbrasives factory around that area? Odd thing to find in the wild.

files-2.jpg - 604kB




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
crystal grower
Hazard to Others
***




Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline

Mood: Puzzled

[*] posted on 7-12-2016 at 08:57


Those crystals may be SiC too. I have similiar sample with small hexagonal crystals in it too. SiC forms 3polymorphs, two of them hexagonal(formed at >1700C) and the last one cubic (formed at lower temp.).
If you have a piece of corund (Al2O3) (sorry if I want much from you :D) you can try to scratch it with this sample, silicon carbide is really hard -about 9.5 in mohs scale.

[Edited on 7-12-2016 by crystal grower]




Elements collected:31/92
Last acquired: Co
Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page
Also make sure to check out my and hegi's website :) :
http://pieceofscience.com
Thanks.
View user's profile Visit user's homepage View All Posts By User
AJKOER
Radically Dubious
*****




Posts: 3026
Registered: 7-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 3-1-2017 at 10:46


I saw a similar rock in a science museum with the bubbles and texture of your mystery rock.

It was presented as a sample of volcanic rock.

So, assuming a lava flow containing hot Si/SiO2 comes into contact with a tree (a source of carbon and CO), the product could be some superficial SiC.

Generally, however, lava is under 1,250 C and may not be hot enough, so the option of an artificial electric furnace formation is still more likely.

Per Wikipedia on SiC (https://en.m.wikipedia.org/wiki/Silicon_carbide ), it is not likely moissanite, as that is an extremely rare mineral.

[Edited on 4-1-2017 by AJKOER]
View user's profile View All Posts By User
explosive eddy
Harmless
*




Posts: 10
Registered: 29-12-2016
Member Is Offline

Mood: No Mood

[*] posted on 4-1-2017 at 21:45
Magnetic?


I found a rock similar to this once it was greenish and porous. Whenever I tested it with a magnet it stuck strongly. My theory is it was a iron meteorite that hit water when it was really hot. I found it next to water and it had quite a few fractures that were clean cut for a rock. Have you tested to see if it is magnetic?
View user's profile View All Posts By User
diddi
National Hazard
****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 5-1-2017 at 01:04


it is definitely not a meteorite. I collect them



Beginning construction of periodic table display
View user's profile View All Posts By User
bolbol
Hazard to Others
***




Posts: 167
Registered: 3-1-2015
Member Is Offline

Mood: No Mood

[*] posted on 26-1-2017 at 13:19


What locality did you collect this from? It would help to identify what it might be.
View user's profile View All Posts By User
Maroboduus
Hazard to Others
***




Posts: 257
Registered: 14-9-2016
Location: 26 Ancho Street
Member Is Offline

Mood: vacant

[*] posted on 26-1-2017 at 14:27


Looks an awful lot like some coarse varieties of pumice I've seen.

At least some pumice does in fact scratch glass.

View user's profile View All Posts By User