-Hi,the german text is nonsense(lie?),R.Escales had the same sulfuric acid and kalium nitrate like we today and therefore was the mix the same
inseparable solid mass in his time like today.
-Why the HNSorbitol? it was proof of strength of the acid or better potency of the Nitrate/SA method.I did it many times and I know,that the strongest
fuming acid has with sorbitol problems.And what I found? That this nitrate/SA method (first publicate by Axt?)is (for Sorbitol)the best .Because is
slow.I keeped the reaction mix frozen for one week without oxidation and the product was solid stuff,not a liquid of lower nitrates like usually .I
did it with fuming acid and it blow after one day in fridge.
-my idea about destillation of Mg nitrate with diluted HNO3 is nonsense( Mg nitrate lose water before it melt by 89 C and acid destilate at 120 C).You
are right I should first read what was written.
-The DCM methods look expensive or it need vacuum destilation.
The DCM metod for the nitrate/SA mix is described by Ledgard.
-I will try the vacuum destillation of Mg nitrate /HNO3 but now I am waiting for the nitrate.
[Edited on 15-10-2016 by Thraxx]
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
Experiment asking answer for question,if the use of Mg nitrate and his doublesalt with Amon.nitrate is able to substitute some part of fuming nitric
acid by the nitrolysis of RDX.
RDX is building by 1:4 -1: 500 ratio with yield by 1:8-1:30 and maximum at 1:26 and optimum temperature 20C .In the range 1:3,5 and 85% HNO3 will
appear the DPT .
// 1:8=140,2 + 504 (=336 ml) HNO3//vol. 1g : 2,4 ml.
Therefore ratio 1:3,2 should make it impossible and therefore the possible activity of nitrates will be visible.
Mg (NO3)2 = m.w.= 148,31 anhydrate
+ 6 waters = 148,31 + 108,12 = 256,43 for hexahydrate.
Mg nitrate hexahydrate was melted and dryied at 165 c and cooled.
Experiments
1)14 g Hexamine into 30 ml (45g)Nitric acid (1:3,2) + melted and cooled on the bottom of the beaker 20 ml of Mg N anhydrate = 5g of product
2)14 g H + 30 ml (45g)Nitric acid (1: 3,2) without Mg nitrate= 4g of product
3) 14 g H + 30 ml Nitric acid + melted 15 ml of Mg nitrate togegther with 15ml Amanium nitrate on the bottom of the beaker = 3g of product
4) 25 ml melted (liquid) Mg nitrate poured into 25 ml nitric acid ,cooled and into this acid gaved 14 g of Hexamine= 0 without product.
Discusion:
Mg nitrate is something like mushroom-it is full of watter and you never know,if is already dry or not yet. If I melt it in the beaker and covered it
with glas, now it steamed up.Therefore is necessary to have it melted in the heat for some time.
Conclusion- application of Mg nitrat for concentration of nitric acid in the laboratory is complicate and not convincing .
[Edited on 15-10-2016 by Thraxx]
[Edited on 15-10-2016 by Thraxx]
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
The Escales method is possible with Mg(NO3)2.
I had 70 g of Mg nitrate and I melted it half an hour at 170 C.There was 50 ml melt and at 100 C I put it into 100 ml of cold H2SO4.The
reaction was a bit fuming,but it was not too bad. After adition it was white warm poridge,it was not clear like KNO3/Sulf.acid.After one h. I put it
into freezer .After one hour there was two layers- very white sulfate on the bottom and not clear,but good separated acid . The acid was about 50 ml
and I was able without problems drain it into other beaker.
I wanted to know what is the acid able to do and therefore I gave it back to the beaker with sulfate and misced there 20 g of
sorbitol. This beaker I want to keep in freezer for one week,but after 24 h. there was two layers and red fumes.I pour it into warm watter and there
was very good separated HNS(poor yield) with higher melting point,because at the RT was it solid.Therefore I expect,that this method is very strong
nitrating way,stronger than KNO3/Sulfuric.
I think and hope,that(vac.) destilation of liquid melt of Mg nitrate and sulfuric acid could give fuming nitric acid of more than 100%
concentration.(with N2O5).
[Edited on 15-10-2016 by Thraxx]
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Quote: Originally posted by Thraxx ![](images/xpblue/lastpost.gif) |
I think and hope,that(vac.) destilation of liquid melt of Mg nitrate and sulfuric acid could give fuming nitric acid of more than 100%
concentration.(with N2O5).
|
Sadly theorically and practicaly not possible to make N2O5 from H2SO4 and Mg(NO3)2...
Think twice to the problem by writting the chemical equations:
1°)Mg(NO3)2.xH2O -heat-> Mg(NO3)2 + MgO + H2O + NxOy
2°)H2SO4 + Mg(NO3)2 --> 2 HNO3 + MgSO4
3°)MgO + 2 HNO3 --> Mg(NO3)2 + H2O
4°)MgO + H2SO4 --> MgSO4 + H2O
You already see that at best you get HNO3 and you may even add water if Mg(NO3)2 was heated too strongly...
Why would N2O5 and H2O split appart form HNO3 and where would the water go? Without P2O5 or SO3 hard to get N2O5...
Maybe B2O3 since H3BO3 + nitrate when heated produces HNO3 of medium concentration and borax ... and B2O3 results from calcinating H3BO3...so maybe
direct heating of B2O3 and nitrate may lead to N2O5?
[Edited on 17-11-2016 by PHILOU Zrealone]
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
Thank you for advice and good idea.N2O5,they write,is solid stuff sublimating at 30 C.If it will retain in cooler,then it could make problems.
I repeated the experiment with Mg nitrate in Escaless method-60 g Mg nitrate hexahydrate was melted at 170 C.It was abbout 25 ml.In
other beaker was 100 ml of cold sulfuric acid.The hot Mg nitrate melt was added to the SA.After one h. was it filtered on vacuum-frita.There was 65 ml
acid.
Now there is a question,what is this acid able to nitrate.But we can say,that this conc. nitration acid was prepared without
destillation.
[Edited on 15-10-2016 by Thraxx]
[Edited on 15-10-2016 by Thraxx]
[Edited on 15-10-2016 by Thraxx]
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Quote: Originally posted by Thraxx ![](images/xpblue/lastpost.gif) |
Thank you for advice and good idea.
N2O5,they write,is solid stuff sublimating at 30 C.
If it will retain in cooler,then it could make problems.
I repeated the experiment with Mg nitrate in Escaless method-60 g Mg nitrate hexahydrate was melted at 170 C (It was about 25 ml).
In other beaker was 100 ml of cold sulfuric acid.
The hot Mg nitrate melt was added to the SA.
After one h. was it filtered on vacuum-frita.There was 65 ml acid.
Now there is a question,what is this acid able to nitrate.
But we can say,that this conc. nitration acid was prepared without destillation.
|
If you know your initial product to be an hexahydrate...this means:
Mg(NO3)2.6H2O --heat--> Mg(NO3)2 + 6 H2O
So for each mole of the hexahydrate, you get 1 mole of Mg(NO3)2 and 6 mole of vapour.
A simple weight loss analysis may give you a good idea at what point of the dehydration you are (assuming you don't overheat to decompose the Mg(NO3)2
partially into MgO and NxOy)
1 mole Mg nitrate = 148.31g
6 mole water = 18g*6 = 108g
1 mole Mg nitrate hexahydrate = 256.31g = 148.31g +18g*6
So 148.31/256.31*100%= 57,86% dry matter = 42,14% weight loss as vapour.
--> Heating but moderate
--> Patience
--> Regular mixing and agitation
--> Regular venting of the above layer with dry/hot air
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
Then I must it all repeat,because if the weight loss is 42%,then it was 34,8g nitrate and there should be not 100 ml sulfuric acid,but 66,9 ml.
But there is the MgO problem.On the bag with nitrate they wrote,that there is 15% of MgO and other MgO will there appear through decomposition
during melting.
15 %of 34,8 is 5,22,therefore it shoud be somethig over 40g nitrate and 15% of acid is 10ml,therefore 77 ml.
[Edited on 15-10-2016 by Thraxx]
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Don't make things more complicate than they look...
You can dissolve the nitrate in the minimum amount of warm water and filtrate...owing to common ion effect, the solubility of Mg(OH)2/MgO what is
already weak, will be even less and thus remain solid onto the filter.
You may also add a slight exces HNO3 to make Mg(NO3)2 out of the MgO/Mg(OH)2...the tiny excess will volatilise during evaporation/crystallization.
--> Many simple solutions.
[Edited on 20-11-2016 by PHILOU Zrealone]
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
Back to the white nitric acid.
I heard about very economic method :One man have vacuum destilation with 4 l bottle and destillate only Nitric 65% + sulfuric conc.First he fill there
2 l sulfuric acid and write the surface.After he put there the nitric acid and destillate.It does he one day and the second day he recovery the
sulfuric acid-he is heating such long,as the surface of sulfuric acid is on the same place like before.
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Quote: Originally posted by Thraxx ![](images/xpblue/lastpost.gif) | Back to the white nitric acid.
I heard about very economic method :One man have vacuum destilation with 4 l bottle and destillate only Nitric 65% + sulfuric conc.First he fill there
2 l sulfuric acid and write the surface.After he put there the nitric acid and destillate.It does he one day and the second day he recovery the
sulfuric acid-he is heating such long,as the surface of sulfuric acid is on the same place like before.
|
Yes economical,
Only noticeable inputs are 65% HNO3, electricity (for vaccuum and heat).
The conc H2SO4 is recycled and thus input = Price H2SO4 conc/number of cycli.
[Edited on 23-11-2016 by PHILOU Zrealone]
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
markx
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 645
Registered: 7-8-2003
Location: Northern kingdom
Member Is Offline
Mood: Very Jolly
|
|
Quote: Originally posted by Thraxx ![](images/xpblue/lastpost.gif) | Back to the white nitric acid.
I heard about very economic method :One man have vacuum destilation with 4 l bottle and destillate only Nitric 65% + sulfuric conc.First he fill there
2 l sulfuric acid and write the surface.After he put there the nitric acid and destillate.It does he one day and the second day he recovery the
sulfuric acid-he is heating such long,as the surface of sulfuric acid is on the same place like before.
|
It is economical as long as you get to the part of concieving a viable vaccuum apparatus for this setup. And forget about practical regeneration of
the sulfuric under atmospheric pressures. If one is not willing to invest top dollar for a chemically resistant vaccuum pump (teflon coated) then the
only other option is a water operated suction pump. Basically all other types of mechanical vaccuum pumps will fail very quickly due to the acidic
vapours discharge from the flask (scrubbers and traps will not help much). Also please consider the matter of safety....I would be extremely cautios
about pulling a considerable volume containing hot sulfuric (up to 300C hot that is) under vaccuum and being nearby at the time. Should that flask
fail for some reason then the results will be catastrophic. And these reasons are numerous...thermal shock, backflush of water from flow pump,
mechanical influence, internal defect in glassware just to name some. Building a failsafe for the ones that you can spot will already complicate the
system to a point that makes it unreasonable for occasional amateur use. I've been contemplating about this matter for quite some time and finally
arrived at the revelation that simple atmospheric distillation of nitrate salt+concentrated sulfuric is the most reasonable approach after all. Truly
the cost in time, money and just plain technical complications is not worth to construct a sulfuric regenerating system compared to the cost of
discarding the acid through the simple salt distillation. It's not like you need gallons of WFNA after all....
Exact science is a figment of imagination.......
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
All what you wrote is true.Grave true. I destilled with vacuum only one time and have a 1 l scrubber with two cocks before and after the scrubber.But
my pump was not too strong.
Conc.sulfuric acid is expensive and may be,that in the future they will it not sell.Possibility to concentrate it from diluted sulf. for cars could be
important.
I did once the concentration of sulfuric ac. in atmospheric pressure and it was a lot of blows and the last blow up was the biggest.Better not
remember.
Perhaps could be good to construct destillation machine from steel with threads,sealed with teflon tape , with two motors ,one for cooler and
second for vacuum.Thermometer external.It could be nice small machine.
[Edited on 15-10-2016 by Thraxx]
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Quote: Originally posted by Thraxx ![](images/xpblue/lastpost.gif) | All what you wrote is true.Grave true. I destilled with vacuum only one time and have a 1 l scrubber with two cocks before and after the scrubber.But
my pump was not too strong.
Conc.sulfuric acid is expensive and may be,that in the future they will it not sell.Possibility to concentrate it from diluted sulf. for cars could be
important.
I did once the concentration of sulfuric ac. in atmospheric pressure and it was a lot of blows and the last blow up was the biggest.Better not
remember.
Perhaps could be good to construct destillation machine from steel with threads,sealed with teflon tape , with two motors ,one for cooler and
second for vacuum.Thermometer external.It could be nice small machine.
[Edited on 15-10-2016 by Thraxx] |
I would go for SO3 production from sulfate salt pyrolysis.
Then add two moles of SO3 (approx 160g) per 100g of HNO3 64%...
HNO3 64% is 64g HNO3 and 36% H2O (or two moles).
HNO3 + 2 H2O + 2 SO3 --> HNO3 + 2 H2SO4 + a lot of heat
(the HNO3 will probably boil off)
The final mix is HNO3 (100%) (64g) and H2SO4 (100%) (196g).
Then distill into glass rod distill apparatus (eventually under mild vaccuum) to recollect the conc HNO3.
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
Pyrolysis of sulfate( Fe2(SO4)3 need over 480C.There is a question,if such work is possible to do in glass.
And if yes,then would be better to sent the smell shortest way (without cooling) into the sulfuric acid for to make oleum.
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Quote: Originally posted by Thraxx ![](images/xpblue/lastpost.gif) | Pyrolysis of sulfate( Fe2(SO4)3 need over 480C.There is a question,if such work is possible to do in glass.
And if yes,then would be better to sent the smell shortest way (without cooling) into the sulfuric acid for to make oleum. |
Pyrex glass resist quite wel heat ... up to melting point thus 480°C is no troubles. Of course normal glass would break due to dillatation
coefficient and resulting stress.
Sulfur trioxide from laboratory process by two-stage pyrolysis of sodium hydrogenosulfate via intermediary sodium pyrosulfate
1°)Dehydration at 315 °C:
2 NaHSO4 → Na2S2O7 + H2O
2°)Cracking at 460 °C:
Na2S2O7 → Na2SO4 + SO3
Procedure is wel documented into the forum.
[Edited on 26-11-2016 by PHILOU Zrealone]
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
markx
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 645
Registered: 7-8-2003
Location: Northern kingdom
Member Is Offline
Mood: Very Jolly
|
|
Calling SO3 into the equation will hardly make things easier from a practical point of view Working with a highly corrosive volatile matter that needs a huge amount of work and custom made equipment to produce is a route that I
would not really want to wander in the amateur realm. I've been involved in a process that produced TiCl4 as a sideproduct and this being vaguely
similar to SO3 in properties I can say that it means the end of basically all materials and equipment that came in to contact with it or the fumes for
any considerable time.
Basically all the methods to obtain WFNA rely on the principle of removing water from the precursor mix or releasing HNO3 via the action of a strongly
water affinic substance. Be it SO3, conc, H2SO4, nitric oxides or Mg(NO3)2. None of the water binding agents are practically regenerable under
atmospheric pressures. This also goes for magnesium nitrate. But out of the bunch the Magnac (magnesium nitrate based method) process is perhaps the
only one that I would consider of any practical purpose for an amateur setup. At least the dehydrating agent there is not a volatile highly corrosive
liquid or gas, but just magnesium nitrate that has been partly freed from its crystal water by vaccuum drying and posesses a huge affinity towards
water because of that. If I remember correctly then it is possible to dehydrate the magnesium nitrate to its dihydate form under vaccuum and heat, but
never to the anhydrous state without decomposing the salt. It is quite cheap to obtain in the hydrated form and poses no trouble storing. Of course
the trouble starts at the vac system again....all of the same old woes return: pump failures, temperature hazards, failure of vac flask, backflush
etc. Also the time spent on the whole experiment is of consideration here....one can fiddle around a complicated "seemingly profitable" method for
months to end up with a mediocre result at a huge cost or just go a simple route and leap to further experiments with the quickly obtained product. So
the question is wether the objective is to obtain WFNA for some further purpose or to study the acid production process itself? If the goal is to
obtain the acid for further experiments, then the simplest KNO3+H2SO4 is definately the practical way to go.....if not, then one can think about
getting involved in the regenerative methods on a level that involves more than just theoretical contemplations. But doing this on any physical scale
truly calls for an expendable facility of its own....forget about performing this in your kitchen. Choose something you can burn down to the ground
with all contents and not mourn the losses.
Exact science is a figment of imagination.......
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
About the nitric acid:
Properties:
HNO3 ,Mr.63,are white crystals,stable below its f.p. or m.p. at – 41 C.at higher temperature take place the slow decomposition :4HNO3
==4NO2+2H2O+O2 .Boiling point for anhydrous acid is at 83-87 C,for aquous (68%)at 121 C. The decomposition is slowly and cause noxes.The higher is the
temperature,the higher are lost of acid and more noxes.
Some authors told,that only Au,Pt , Cr steel and Al are stable in the fuming nitric acid.Other autors told,that iron is stable too.(?)
Manufacture:
Either we manufacture the nitric acid or we concentrate it.And between are clever pathways which combine this two sources of fuming nitric acid for to
optimalising the waste problem how to throw the sulfate out from the bottle.
Simultaneously or after we have the fuming acid can we use one of three ways to the wanted white fuming nitric without noxes-adding urea,air bubbling
and vacuum preparation of step I.
I. Glaubers fuming nitric acid 1648
-heating 85 parts kalisalpeter with 98 parts sulfuric acid below 150 C to avoid loss by decomposition of the nitric acid.(Kalisalpeter was there to
y.1900,after was it Chilesalpeter.)(1)
I. – 1- manufacture:
Theoretically:
NaNO3 + H2SO4 == NaHSO4 + HNO3
Mr=85 98 120 63
53,6ml 42ml
mp=306,8C 58,5C
KNO3 KHSO4
Mr=101 136,17
mp=334C 197 C
NH4NO3 NH4HSO4
Mr=80 115,11
mp= 169,5 C 121-145C
In the praxis today there was described these rations:
900 g KNO3 + 500ml H2SO4 (2)/need 22ml SA/
400 g NaNO3 + 500ml H2SO4 == 150-200 fuming NA after 2,5 h destillation (3)/remain 252ml SA,could be added 144ml nitric ac./
68 g KNO3 + 32 g H2SO4 (4) /need 4 ml SA/
58 g NaNO3 + 32 g H2SO4 destilled at temperature 80-90C (5)
(to the NaNO3-could be manufactured from Ca(NO3)2 and Na2CO3 and give 15% more HNO3 than KNO3)
80 g NH4NO3 + 100 g H2SO4 = unsatisfactory concentration (1,22 g/cm3)(6)
80 g NH4NO3 + 100ml H2SO4= unsatisfactory concentration,doesnt work with hexamin(7)
The waste beginn to crystalise after 10 min after heating.It is necessary to disassemble the distill. Ap.
I. 2 : Concentration of nitric acid to highest concentration:
- Frenchman and Rouelle 1750- concentration of weak nitric acid with conc. sulfuric acid by distillation.
Today ration:
200ml 65% HNO3 + 350ml 96% H2SO4 at 110-120 C give 108-110 ml fuming NA
280g 640,5g
of 1,51g/cm3 (8)
( spent acid is 440 ml of 72% sulfuric acid,therefore was used 3,57ml conc. sulfuric acid for every ml of watter in the nitric acid or 1,75ml
sulfuric acid for every ml of nitric acid.In according to Valentiners proces it schould be 280gNA : 560 gSA)
-concentration without distillation with help of anhydrous magnesium nitrate or calcium nitrate:
- Escales method of cold separation of misced nitric and sulfuric acid-although by author described method with Na or K nitrates (1 weight part of Na
or K nitrate + 31/2 weight part of conc. sulfuric acid cooled at 0 C and separate )was impracticable,but there was found an other way with anhydrid of
Magnesium nitrate. (9)
- Valentiners vacuum proces-19.century(Basil Valentinus lived in 17.c.?)Distillation at 15-25 mm Hg.
Today:
Laboratory preparation of 99%+
1 part of HNO3 (1,4 g/cm3) +2parts of sulfuric acid (1,84g/cm3)dist. under vacuum.(10)
Combined methods:
140ml 65%HNO3 +170ml 96% H2SO4+70g NaNO3== 110ml fuming NA(11)/there should be 72 ml HNO3/
350 g NaNO3 + 500ml H2SO4 + 150 ml HNO3== 200-250ml fuming NA(12)/there should be 18ml SA less/
I. 3 : Extraction of nitric acid with DCM -20.century like patent 549198 or 3981975.Ledgard described manufacture of absolute nitric
acid : 94ml sulfuric acid +106 ml 70% HNO3+ extraction 7x 200 ml DCM and after this vac.destillation of DCM. (13)
II.-White fuming nitric acid – because the Noxes are allowed to 4% and more could make explosion of hexamine or oxidation of other
reaction,is better to have NA without noxes.
-Bubbling ,air gurgling (14)
-vacuum destilation (Valentiners proces)
-adding of urea –1)hot-should be at 60 C but it is very exothermic reaction with some delay.Adding
10g of urea into 250 ml fuming NA for 15 min need to wait 2 h for to be sure,that the reaction is ended.During adition are huge amount of noxes
outgoing,which could do explosion and are highly toxic .(15)
2)atRT-the same reaction like hot adding,can explode.(16)
3) cold urea -for every 100ml nitric ac. 2 g urea at 0 C-outgoing are CO2
and N.(17)
- boiling - stupid like hot adding of urea .
III.-Fuming nitric in situ:
-Different methods of nitration with sulfuric acid and nitrates Na,K, or Ca (18)
------------------------------------------------
Numbers (1)to(18) are numbers of pathways
------------------------------------------------
What I allowe me to suggest is 1) iron distillation apparatus and 2) one iron flask with pipe for cracking of NaHSO4 (destillation waste).
The iron apparatus should have two iron flasks connected through threads with long pipe of U shape which one arm is going through watter bath
.Connected to strongest vacuum pump.
Questions about waste:
To the waste,called "nitro cake"-if it is NaHSO4,could it react with Ca(CO3)2 to NaNO3??
-at how temperature will be possible reaction: NaNO3 + H2SO4 ==Na2SO4 + 2 HNO3 if it will be done
under vacuum?
At atmos. pressure it isnt possible,because the temperature is need too high and the HNO3 will be decomposed to noxies.But under vacuum? This reaction
need only half of amount of sulf.acid and the nitrocake could be converted with Ca nitrate.
[Edited on 15-10-2016 by Thraxx]
[Edited on 15-10-2016 by Thraxx]
[Edited on 15-10-2016 by Thraxx]
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
@Thraxx,
Iron becomes passivated by contact with conc HNO3 alone...but contact with other metals may deactivate the passivation; I don't know what happens when
lower % HNO3 is involved nor what happens when conc HNO3 and H2SO4 are together into contact with iron.
QUOTED From you:
"To the waste,called "nitro cake"-if it is NaHSO4,could it react with Ca(CO3)2 to NaNO3??"
1°) Ca(CO3)2 doesn't exist, it is CaCO3...Ca is bivalent and H2CO3 is diprotic acid.
2°) If it is NaHSO4 then reacting it with CaCO3 will never make NaNO3...that would call for nuclear chemistry (transmutation of one atom into another
... C into N)
Wait! I read into your mind...![;)](./images/smilies/wink.gif) ![:P](./images/smilies/tongue.gif) ![:D](./images/smilies/biggrin.gif)
--> I guess you meant Ca(NO3)2 instead of Ca(CO3)2
Indeed:
NaHSO4 + Ca(NO3)2 --> CaSO4(s) + HNO3(v) + NaNO3
Because transciently:
2NaHSO4 <==> Na2SO4 + H2SO4
so
Na2SO4 + Ca(NO3)2 <--==> CaSO4(s) + 2 NaNO3
H2SO4 + Ca(NO3)2 <--==> CaSO4(s) + 2 HNO3 (v)
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
If we havent KNO3 more and if we have a lot of time and money,then could we do this manner:
Distillation:
Ration: 500 ml H2SO4 (915g=9,33 mol)+ 950 g KNO3 (9,33 mol)
The nitro cake will have 1270 g and need to throw it out from bottle either like solid or with 3 l of hot watter to other bottle of 10 l
volume.There add 2203 g of Ca(NO3)2 in 2 l hot watter and after some hours add there solution of 500 g KOH in 1l watter . After a longer time for
decantation of plaster of paris there could be solution of 1884 g KNO3 in 6000 ml watter,which need to be evaporate.
DISTILLATION :
KNO3 + H2SO4 == KHSO4 + HNO3
Mr= 101 98(53,6ml) 136,17
mp= 334C mp=197 C
solubility= 49g/100ml at 20 C
WASTE-NITRO CAKE:
KHSO4 + Ca(NO3)2== HNO3 + KNO3 + CaSO4
Mr=236,15/tetrahydrate/
m.p.=42,7C
Solubility =444,3g/100ml at 20 C
Neutralisation:
HNO3 + KOH ==KNO3 +H2O
Mr=56,1
m.p.=406 C
Solubility= 121g/100ml at 20 C
----------------------------------
Today I did the "white fuming nitric"-
Some days ago I distilled NaNO3 + SA at vacuum-there stood something like stone from NaNO3,because the low vac.temperature was unsufficient for the
reaction .So I added there new SA + nitric acid and distillated it at atm pressure. It worked well,but there was amount of brown noxies and the
fuming acid was dark yellow.
First I cold to O C in ice bath and added there 2g urea for 100 ml of acid.What happened? nothing,no fumes,no bubbles it diluted mild and easy
and the acid stood yellow.
I found it unsufficient and put there an air through glass pipe.It was good pressure,acid gurgled in the bottle and really a lot of fumes
,White fumes get out.It was a few minutes,may be 5 min. and after it gurgled but there was the white fume no more.And the acid stood yellow.
Before I ever throwed urea to warm acid with gasmask,respirator was unsufficient.Acid squirted out of bottle and there was a very much of brown
fumes .And the acid was then really like watter.It was total bad -I decomposed me my acid.
It seems me,that right was the method of cool bubbling,and the bad noxies diluted in HNO3 are the white fumes and not brown fumes,which are
from decomposed HNO3.And the acid may be yellow.
---------------------------------------------------------
If the Sulfuric acid need to be concentrate,then perhaps could be such way:
Generally:
- Sulfuric acid H2SO4.Mr= 98,m.p. 10,36 C ,boiling point 273 for 100% and 310-335 for 98 %,Decomposition up 338C.
- SO3-melting point 16,8C,boiling point 44,8C
- KHSO4-melting point 197 C,boiling point with decomposition 300 C
- K2S2O7-mellting point 325 C and decomposition between 460 up to 600C
1. Step- making Potassium hydrogensulfate through Distillation at higher degrees to 150 C of KNO3 800 g + H2SO4 500ml== KHSO4 1078,5 g + H2SO4 in
one bottle and HNO3 + noxies in the second bottle which we turn for other bottle with Sulf acid which should be concentrate .
2.Step- making Potassium pyrosulfate through heating.
-At 240 C there will be decomposition to K2SO4 +H2SO4,but the sulf.acid should stay in the bottle.
-At 320 C there will be decomposition of sulfate to pyrosulfate :
2 KHSO4 ==K2S2O7 + H2O
…and the sulf.acid will distillate,but it must stay there like catalysator.
3. Step-pyrolysis of pyrosulfate at 460 C .First melt the pyrosulfate and after boiling are white fumes of SO3 outgoing from melt to cooler.
K2S2O7 == SO3+ K2SO4
Video here:
http://www.prepchem.com/synthesis-of-sulfur-trioxide/
[Edited on 15-10-2016 by Thraxx]
[Edited on 15-10-2016 by Thraxx]
[Edited on 15-10-2016 by Thraxx]
[Edited on 15-10-2016 by Thraxx]
|
|
markx
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 645
Registered: 7-8-2003
Location: Northern kingdom
Member Is Offline
Mood: Very Jolly
|
|
Thraxx....you need to do a bit of fraction cutting during the simple acid distillation. Majority of nitric oxides come over in the "heads" or the
first fraction that boils over. It is mostly less than 10% of the total acid yield. You need to collect these nitric oxide rich heads separately and
discard. The rest of acid comes over quite pure after that. It will still have a slight yellow hue to it, but that is not a problem for nitramines in
direct nitrolysis route and even less in Bachmann route. The urea addition makes quite a mess as you can conclude from your previous experienece. Also
there is no need to really go slow with the distillation....as long as you separate the first bad fraction, you can turn up the boil rate and run
quite fast. That is provided your flask and other equipment can handle the thermal shock with no trouble. I suggest you do not use an oil bath to
heat the acid flask.....if it breaks then the resulting mix will most definitely burst into a raging fireball. I have found that hanging the flask
directly over a hotplate, but not in direct contact is perhaps the safest way to do it when using glassware.
Exact science is a figment of imagination.......
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
@Thraxx,
Na pyrosulfate is better than K pyrosulfate to make SO3... the K version favors decomposition of the SO3 into SO2 and 1/2 O2...so yield will be lower
/amount will be less.
[Edited on 1-12-2016 by PHILOU Zrealone]
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
Microtek
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 849
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
In the EU, sulfuric acid is becoming a restricted chemical in concentrations above 30 or 50 %, so the ability to produce or recycle is more
important than ever.
I have experimentet with boiling down dilute sulfuric at atmospheric pressure and obtained acid of ca. 90-93 % concentration without exceedingly high
temperatures or particularly long heating time.
While this concentration is not as high as would be preferred, it is still high enough for concentrating dilute HNO3 (though you may need more than
one distillation).
Of course, nitric acid is also becoming restricted (above 10% IIRC), so that is another chemical that will be necessary to produce.
|
|
Thraxx
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 71
Registered: 15-10-2016
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Microtek ![](images/xpblue/lastpost.gif) |
I have experimentet with boiling down dilute sulfuric at atmospheric pressure and obtained acid of ca. 90-93 % concentration without
exceedingly high temperatures or particularly long heating time.
|
If I understand,you didnt boil the acid,you only heated and for the concentration or evaporation it was sufficient?
|
|
Microtek
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 849
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
No, I did boil it, but it wasn't at an extremely high temperature. I simply heated it strongly until the temp reached somewhere around 200 C. Then