Production of nickel, copper and silver as potassium cyanide
I have successfully produced very pure PGC by electrochemical preparation by using 40gpl of KCN as both the anode and cathode solution.
The anode was a 24k pure gold foil, the cathode was a 304 Stainless steel inside a porous cup. Voltage was around 12v.
Upon anode disintegration, the anode solution was boiled down to 25% volume, as the solution cools very white PGC precipitated. Washed with very cold
water three times and was vacuum dried.
Now I wonder if the same procedure will work for Nickel, Copper and Silver? As their potassium cyanide salt form is not readily available in my
country I have to prepare them myself.
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
PGC? Potassium Gold cyanide?
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
autumnwilow
Harmless
Posts: 2
Registered: 23-11-2016
Member Is Offline
Mood: No Mood
|
|
Yes, exactly.
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
Silver I think yes. I don't know about the others.
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4296
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
K2[Ni(CN)4] is easily made by reaction of KCN with nickel cyanide (itself easily made by reaction of any soluble nickel salt with two equivalents of
potassium cyanide).