Separating Bismuth Powder From Aluminum
I am trying to extract bismuth from Pepto Bismo using the HCL and aluminum procedure, but I ended up with a pile of bismuth powder mixed in with
aluminum. The aluminum pieces are too small and brittle to manually remove and I think around 40% of the powder is aluminum.
Does anyone have any suggestions on how to separate the two metals so that I end up with mostly bismuth?
Thanks.
|
|
Jstuyfzand
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 166
Registered: 16-1-2016
Location: Netherlands
Member Is Offline
Mood: Learning, Sorta.
|
|
Maybe Sodium Hydroxide to dissolve the Al?
I dont know what it will do to the bismuth though
|
|
pinkamena
Harmless
Posts: 2
Registered: 23-8-2016
Member Is Offline
Mood: No Mood
|
|
You could just throw the whole mixture into hydrochloric acid, aluminium will dissolve because it's electropotential is below that of hydrogen (Al3+ +
3e- > Al : -1.7V), and bismuth will remain because it's electropotential is above that of hydrogen (Bi3+ + 3e- > Bi : +0.4V).
|
|
mayko
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1218
Registered: 17-1-2013
Location: Carrboro, NC
Member Is Offline
Mood: anomalous (Euclid class)
|
|
Did you shred the aluminum? I've seen some preps do this but I've precipitated bismuth just fine with an aluminum foil sheet corrugated into a fan,
with minimal aluminum contamination
al-khemie is not a terrorist organization
"Chemicals, chemicals... I need chemicals!" - George Hayduke
"Wubbalubba dub-dub!" - Rick Sanchez
|
|
mesanaw
Harmless
Posts: 10
Registered: 29-10-2016
Member Is Offline
Mood: No Mood
|
|
I just stirred the solution with a large piece of aluminum and then let it rest in the container. I'm going to try washing it with dilute HCL and
hopefully that will work.
It worked perfectly. I have some really clean-looking powder thanks everyone!
[Edited on 29-10-2016 by mesanaw]
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
The real trick is turning that powder into a solid ingot of metal! Because of its high surface area, it oxidizes to yellow bismuth(III) oxide instead
of melting when heated. I tried a few tricks to get it to melt but never could. Now that I have an argon cylinder, it might be worth looking into
again.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
I managed to do it with cadmium powder and copious amounts of NaOH flux, so it should be possible.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 514
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
Here is a video of Nile Red getting bismuth metal into an ingot from powder that he extracted from pills. He says that strong heating of the bismuth
oxide will decompose it back into bismuth metal and oxygen.
https://www.youtube.com/watch?v=grpSfjUImUs
|
|