Author: Subject: Zinc Chloride Strange Floaters
Meltonium
Hazard to Self
**




Posts: 97
Registered: 23-9-2016
Location: Home in pajamas
Member Is Offline

Mood: Fluorinated

[*] posted on 21-10-2016 at 13:13
Zinc Chloride Strange Floaters


Currently, I am dissolving some solid zinc I obtained from electrolysis of ZnO into some hydrochloride acid. As the reaction proceeds, I notice more and more of these black "floaters." They resemble eraser shavings in size and shape except that they are black. At first, I thought they were just little bits of zinc that were floating on the rise of H2 bubbles, but it doesn't seem like they are dissolving. What are they?
View user's profile View All Posts By User
Maroboduus
Hazard to Others
***




Posts: 257
Registered: 14-9-2016
Location: 26 Ancho Street
Member Is Offline

Mood: vacant

[*] posted on 21-10-2016 at 13:47


I have seen much the same thing when dissolving a zinc anode in HCl, but never noticed anything like it when reagent grade mossy zinc gets dissolved in HCl, so i assume it's from impure zinc.

Where did that Zinc oxide come from?

Seems to me zinc is one of those metals like lead that tends to have a lot of other stuff in it unless it's rigorously purified.

[Edited on 21-10-2016 by Maroboduus]
View user's profile View All Posts By User
Meltonium
Hazard to Self
**




Posts: 97
Registered: 23-9-2016
Location: Home in pajamas
Member Is Offline

Mood: Fluorinated

[*] posted on 21-10-2016 at 14:19


Quote: Originally posted by Maroboduus  


Where did that Zinc oxide come from?


The ZnO was only pottery grade, so you're probably right about the impurity, but I'm curious to know what this impurity is.

[Edited on 21-10-2016 by Meltonium]
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 21-10-2016 at 20:02


How did you electrolyze your ZnO? I assume you dissolved it in some acid first. Did it all dissolve then?



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Meltonium
Hazard to Self
**




Posts: 97
Registered: 23-9-2016
Location: Home in pajamas
Member Is Offline

Mood: Fluorinated

[*] posted on 22-10-2016 at 09:32


Quote: Originally posted by Metacelsus  
How did you electrolyze your ZnO? I assume you dissolved it in some acid first. Did it all dissolve then?


Dissolved in NaOH, but I didn't have all of it dissolve.
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 22-10-2016 at 15:01


In that case, I hypothesize the floaters to be something that dissolved in the basic solution, got reduced along with the zinc, and did not dissolve in the acid. In that case, it could be metallic lead from PbO in the ZnO. Lead doesn't float, but there might be trapped hydrogen gas causing it to rise.



As below, so above.

My blog: https://denovo.substack.com