wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
Cheap titanium sheet on ebay
£2 for Ti Foil-0.1mmx100mmx300mm
http://www.ebay.co.uk/itm/Titanium-TC4-GR5-Ti-Thin-Plate-She...
|
|
Jstuyfzand
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 166
Registered: 16-1-2016
Location: Netherlands
Member Is Offline
Mood: Learning, Sorta.
|
|
Nice!
Nickel goes cheaply too!
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
It's GR5 Ti alloy, which means 90% Ti, 6% Al, and 4% V. Just so everyone's aware of that.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4547
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
You're welcome
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1477
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
A tip for people scoring Ti and alloys on ebay: get the size you want, unless it's thin enough to cut easily. My dremel with thin cut off disks was
having a hellofa time cutting 1/16" sheet. Several (5) to cut about 7 linear inches.
I saw the cost of some thicker plates and sheet, like 1/4" - 1/2", thought it was a bit much compared to larger blocks. I then noticed some big
blocks going for a relatively low cost for the amount of Ti presented. So reasoned I could get bigger blocks, take to the local machine shop and have
them slice it like bread, sell off a few to cover costs. Leaving me with basically free material of my choice size. Deffinitely NOT how it worked
out.
The machine shop guy said no way, but he could order what I wanted. Otherwise it was necessary to find a hydrojet equipped shop, pay by the inch,
weeks of wait time and then try to recoupe my costs... So I have $100 worth of Grade 5 (6-Al,4-V) sitting on a shelf. somewhere near 16 lbs, a
respectable sum for the two blocks pics are fourth post down- https://www.sciencemadness.org/whisper/viewthread.php?tid=26...
I did call and the nearest hydrojet guy was a little over an hour away, charged $3/in and had a two week wait time. Maybe I'll think of something to
use it for worth the time/cost one of these days... so bear in mind it isn't something easily parted out or fabricated in general for an amateur w/
limited tools and money.
-VS
|
|
diddi
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
if you are collecting. go for Gr1 or sponge if you can find any. and buyer beware of getting fake purity out of china. there are good suppliers in CN
but they are not on ebay
[Edited on 15-10-2016 by diddi]
Beginning construction of periodic table display
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Is it possible to anneal the stuff to soften it up?
if you want to make electrodes from it softening it would make it easier to cut to shape.
|
|
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
I thought TC4 was low oxygen and considered commercially pure Ti. I failed to find any reference for GR5.
I checked some different references and you are correct about the composition. I guess that aluminium would reduce its corrosion resistance. How
suitable it is for electrolysis or molten metals I do not know.
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
I have 1.5 mm sheet CP grade 2 that I can shear to size for whomever wants. Used to have a lot more but sold most all of it. Regretting that now.
$10/square foot + shipping and $1.50/cut (it does work harden and I have to sharpen the shear blades).
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
yobbo II
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 728
Registered: 28-3-2016
Member Is Offline
Mood: No Mood
|
|
http://www.ebay.co.uk/itm/Titanium-TC4-GR5-Ti-Thin-Plate-She...
Gr5 (Grade 5) is in the listing name.
Grade 2 here
http://www.ebay.co.uk/itm/Titanium-Ti-Gr2-Grade-2-ASTM-B265-...
This thickness of stuff is too thin as cathodes and has failed when used in chlorate etc cells
Canadian supplier here
http://www.ebay.com/itm/Titanium-Foil-Sheet-005-13mm-x-10-25...
Search for grade 2 titanium foil
[Edited on 17-10-2016 by yobbo II]
|
|