Any interest in a palladium-based catalytic chemistry kit?
I recently discovered I had some money in a precious metals trading account that I'd forgotten about, and used it to buy an ounce of palladium. Of
course, I don't need that much palladium, so I've started dissolving it to get the chloride salt, since that's the only way I can conceivably divide
it up.
I plan to sell it on eBay, where it's been going for about $40 a gram, but I figured I'd check interest here too. Obviously, you guys could buy it
for a significant discount. I could also include carbon black, copper chloride, nickel sulfate, graphite electrodes, activated alumina beads, a
hydrogen-generating aluminum alloy (just add water), and potentially other reagents that are useful for palladium chemistry. I'm open to other ideas
for things I could add to a palladium chemistry starter kit too. Incidentally, I'm using only chemicals from a local jewelers' supply store, so this
won't be dissolved in hardware-store muriatic acid or anything.
Palladium is probably one of the easiest, most useful metallic catalysts to use, since it can perform catalytic hydrogenation (as well as oxidation)
at ambient or near-ambient pressures, and does so more readily than the other two popular hydrogenation catalysts: platinum oxide and Raney nickel.
It's also the cheapest platinum group metal that has wide application for use, and can be easily plated onto electrodes to make them inert to common
electrolysis conditions. When looking up catalyzed reactions that could potentially be of use to me, palladium comes up more frequently than any
other element, at least at pressures and temperatures that are achievable in a home lab.
So, is there any interest in a palladium-based catalytic chemistry kit, and if so, what would you like to see in one? I'm open to suggestions, and
also open to trading said kits for reagents and/or equipment. I plan on using any money I make to investigate non-toxic alternatives to reactions
that currently necessitate the use of mercury, so non-toxic metals that are components of low-melting-point alloys would be particularly appreciated
as part of any exchange. Gallium and indium in particular, since they're the most expensive.
|
|
MediMan
Harmless
Posts: 1
Registered: 23-8-2016
Member Is Offline
Mood: No Mood
|
|
PdCl2
Hey, I'm interested. In some of the PdCl2
How can we arrange the exchange?
|
|
Melgar
Anti-Spam Agent
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline
Mood: Estrified
|
|
The only issue with doing the exchange right now is that I'm currently lacking nearly all of my lab equipment, including my milligram scale. However,
I do have 500 mL of dark brown PdCl dissolved in acid! I figured a fair price would be $30 for the first gram of PdCl2, $25 for each gram after that,
and a grab-bag of various useful things including but not limited to:
~4 oz. of activated alumina beads, about 1/8" in diameter
A bobbin of PTFE thread, useful for sewing electrolysis membranes and a number of other things.
An appropriate amount of carbon black for loading with Pd
CuCl2 hydrate (or anhydrous, if you prefer)
Algalinstan, a cheesily-named alloy capable of generating hydrogen at a fairly consistent rate, at a neutral pH when immersed in water or
alcohol. Metal can be filtered and stored for later when hydrogen is no longer needed.
Strong-base ion exchange resin (I have too much, ok?)
Possibly other reagents, if I can think of them and they don't cost too much to ship.
I'll probably have to limit this to just the US, since even shipping to and from Canada is a pain. Payments can be via Paypal, Bitcoin, or an
equivalent value of useful reagents.
|
|
Arg0nAddict
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 54
Registered: 8-6-2016
Location: PNW
Member Is Offline
Mood: Mercuric
|
|
You did buy at a bad time but save it. With us troops surrounding russia I bet metals skyrocket. I took a just below break even on gold chloride
because nobody believed it I. had to have it tested which didn't cost much since they knew exactly what to compare. Still so sales. Then I tossed in a
free gram of silver and that got things going. Weirdly. Personally I never Destroy coins or bars connected to a country becusee they hold more value
what I look for are the home made shitty ingot and work up from there. I have a thing for coins though and I prefer silver. Nothing pretty like a
sealed and never circulated walking liberty. Proof coins are nice but seem fake to Me even though I know they are not, the natural look of a coin
just minted is a favorite. I'd be interested in trading I just spent all on inventory
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
I received the 10%Pd/C gratis from Billy in LaJolla a few days ago as promised (see my post in Preparation of Succinic Acid). As
suggested by Dr Bob, today I tested its activity using methanol. Then I tested it using propane. The results were negative. My son made three short
movies of this testing. So, from the studios of Mr Ardipithicus, here they are:
https://youtu.be/enEykN7nbsQ
https://youtu.be/PSTSCmskPd0
https://youtu.be/lCDD7KWRaB4
As indicated in the last movie, if you have any suggestions for further tests, or corrections to my tests, please let me know.
[Edited on 14-10-2016 by Magpie]: reposted last video - seems to work OK now.
[Edited on 14-10-2016 by Magpie]
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
I would love some Pd/C! Pt I have, but only as a metal. Pd I would like to have as a catalyst on carbon. Looking forward to doing some reductions.
Is there any way to re-activate Pd on carbon? I made some grams about 10 years ago. I'm not to sure about the activity though as I never tested it,
and I'm quite sure it is not active anymore either.
[Edited on 14-10-2016 by Tsjerk]
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
It dawned me that the sulfur gas in the propane might be poisoning the catalyst. But that doesn't account for the failure to ignite the methanol
(Heet).
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
madcedar
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 116
Registered: 10-9-2009
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Magpie ![](images/xpblue/lastpost.gif) | I received the 10%Pd/C gratis from Billy in LaJolla a few days ago as promised (see my post in Preparation of Succinic Acid). As
suggested by Dr Bob, today I tested its activity using methanol. Then I tested it using propane. The results were negative. My son made three short
movies of this testing. So, from the studios of Mr Ardipithicus, here they are:
https://youtu.be/enEykN7nbsQ
https://youtu.be/PSTSCmskPd0
https://youtu.be/lCDD7KWRaB4
As indicated in the last movie, if you have any suggestions for further tests, or corrections to my tests, please let me know.
[Edited on 14-10-2016 by Magpie]: reposted last video - seems to work OK now.
[Edited on 14-10-2016 by Magpie] |
I'm glad to see you got the plastic wrapper off the bottle. ![:D](./images/smilies/biggrin.gif)
You could try what you are doing in reverse. Put a tiny bit of methanol into a beaker with a watch glass on top and allow some time for a methanol
vapour/air mix to form. Remove the watch glass and sprinkle in a tiny amount of catalyst from your spatula. The result should be glowing catalyst
particles, methanol bursting into flames and a potential cardiac arrest. I'm not saying it's a safe test.
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
Magpie,
Those Pd/C catalysts usually only set stuff alight after they've been saturated with hydrogen.
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Good to know! Thanks.
Could this be done be purging the bottle with H2 then keeping it under H2 balloon pressure for some time?
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
That should do it.
One customer has a palladium catalyst that contains about 700 lbs of palladium on 15 tons of carbon. When they discharge it from the reactor it has to
be passivated for months with oxygen to remove absorbed H2. It's a common practice!
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
Morgan
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1675
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
Pd 1.25% on carbon rod bits, and Pd 0.5% on alumina pellets - the two on the right in both photos will both heat up if misted with methanol from a
finger pump sprayer. But if you drench them in alcohol, they don't get a chance I think because the air can't get to them as much. These bits and
pellets made the petri dish way too hot to hold if you placed it in the palm of your hand but they never glowed in this environment and they are slow
to heat up.
http://www.sciencemadness.org/talk/files.php?pid=202104&...
http://www.sciencemadness.org/talk/files.php?pid=202104&...
Better perspective of the Pd pellets.
http://www.pulse-jets.com/phpbb3/download/file.php?id=13733&...
As an aside some 1% platinum on alumina powder.
https://www.youtube.com/watch?v=h3lS3TBuntw
One thing you might try to get palladium on carbon to get going is to heat it strongly and then let it cool down to room temperature and then try to
mist it with some methanol. Sometimes this will activate it. You might try just putting a little methanol on it and lighting that and let it cool.
There's a platinum catalyst lighter that sometimes exhibits this quirky property if it's sat without use for some time. Also if it's very humid out
this can slow the effect of my platinum on alumina powder when sprinkled into a jar containing methanol vapor, the tiny dust particles don't glow red
hot as quickly. And methanol that has absorbed too much moisture from the air will often leave a watery residue say if you burn some on the pavement
and that can inhibit the pellets. This is also true with the Pt catalyst lighters, the methanol saturated cloth/wick eventually builds up humidity
either from combustion or just being repeatedly exposed to the air - the wick will be plenty moist but not as perky as fresh methanol in getting an
ignition to take place, but I digress.
I recall wishfully trying propane with my platinum catalyst and it was a no go if starting from room temperature. But Pt or Pd can ignite hydrogen
this way.
https://www.youtube.com/watch?v=I45xfo-JvTk
One last tidbit from the past.
Expt. 81. Absorption of Hydrogen by Palladium.—One of the simplest ways of causing palladium to absorb hydrogen is to decompose acidulated water by
means of a voltaic current, whereby two gases are evolved—hydrogen at one pole or electrode and oxygen at the other. If the terminals of the wires
leading from the voltaic battery are made to be strips of thin palladium foil, the strip attached as the " negative " electrode, at which the hydrogen
is disengaged, will absorb most of the liberated gas, and in so doing will increase somewhat in dimensions, the metal swelling as it absorbs the gas,
much as water does when it absorbs ammonia (Expt. 74). When a strip of palladium foil, or a thin palladium wire, is fully charged with hydrogen in
this way, a slight elevation of temperature suffices to expel a little of the occluded gas; in consequence the charged metal can be used as a candle
or torch; when the end is held for a moment to a light the heat expels some of the hydrogen, which takes fire and burns ; the heat thus produced
causes morehydrogen to be liberated, so that the flame keeps burning for some time, the metal being clothed with a very pale flame, almost invisible
in daylight, somewhat as though it had been dipped in strong alcohol, and then fired before the spirit evaporated.
http://www.sciencemadness.org/talk/viewthread.php?tid=16329#...
[Edited on 16-10-2016 by Morgan]
|
|
Magpie
lab constructor
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline
Mood: Chemistry: the subtle science.
|
|
Thanks for this Morgan. I will try some misting.
The single most important condition for a successful synthesis is good mixing - Nicodem
|
|
Dr.Bob
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2690
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: No Mood
|
|
I have seen Pd/C set MeOH on fire a few times. Most times were before hydrogen touched catalyst, and with old bottles. Often the catalyst is
shipped wetted with water, and will dry over time, so perhaps let a sample of the catalyst sit out somewhere fire safe and dry overnight, then try it.
10% is much more reactive than 5%, much more than twice as likely to catch fire.
The challenge is that it was not done on purpose, so hard to rreplicate perfectly, but the idea of putting a small amount of MeOH in a beaker, waiting
a while, and then adding a small amount of pd/C to it sounds like what was done wrong. I often weight the catalyst first, then purge with N2, then
add the ethanol solution of compound under inert gas. If the reaction is complex, I might have to add the Pd/C last, in which case I make sure the
solution is well purged/sparged with N2 first, then add the catalyst (preweighed in a vial in one quick portion under N2. But just try the catalyst