Removal of sticky stuff
I have a stereo net encased in plastic. Really the whole thing is polymer. For field work I taped clear vinyl over the nets; they rotate. Now I want
to use it with tracing paper and I've been going at the old tape (scotch tape) with MeOH. I'm afraid to try stronger solvents for fear of losing the
inked graduations or damaging the surface, If it gets roughed up it won't work as well. I don't know the plastic. If I did I wouldn't be asking. I
could try various solvents along the edge somewhere. Before I do that I'd like to now whether other have been in similar situations and if so if
something worked and what it was. I'll try a few detergents before more solvents. Thanks in advance, CRX
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
NedsHead
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 409
Registered: 9-12-2014
Location: South Australia
Member Is Offline
Mood: No Mood
|
|
When it comes to sticky stuff Kerosene always works for me, try a small area first
|
|
ahill
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 57
Registered: 8-1-2015
Member Is Offline
Mood: triumphant
|
|
Vegetable oil.
This is definitely a "Life pro tip".
Olive - peanut - whatever - its great for all kinds of sticky tacky gluey label stuff - coat it on - rub it in - and wait. Hours are better than
minutes, and days better again - dont be afraid to reapply, and when everything is soft enough, wash it off with warm water. Very effective and very
gentle to almost all surfaces.
*I'm a fanatical re-cycler of jars, bottles and other containers.
|
|
RogueRose
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1590
Registered: 16-6-2014
Member Is Offline
|
|
goo-gone or D-limonene I heard works well.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3632
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
I would be very careful if there is exposed ink,
... kerosene for example easily removes many inks,
other solvents may deteriorate the plastic,
isopropanol is mild enough for plastics and most inks,
but I did once remove blue ink from a fascia with it ![:mad:](./images/smilies/mad.gif)
the safest is water and mild detergent but check the manufacturers literature and website first.
Remember ... if all else fails, read the instructions.
P.S. had to google 'stereo net' ... probably not for me in this lifetime
[Edited on 7-9-2016 by Sulaiman]
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
zed
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Ummm.
Do this all of the time with books.
Best solvent....lighter fluid! Handy dispenser.
Sold everywhere. Dries fast, stain-free, and odorless. Works well on tape and sticker adhesives.
|
|
Maroboduus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 257
Registered: 14-9-2016
Location: 26 Ancho Street
Member Is Offline
Mood: vacant
|
|
Have you tried checking with the good folks at 3M? Bet they've got scotch tape adhesive removal advice somewhere on their site.
What I would try first would be dishwashing liquid WITHOUT water. See if it'll break the glue down with light scrubbing, then only add water after it
emulsifies the glue. This works with a lot of highly polar kinds of gunk.
|
|