hippo
Harmless
Posts: 26
Registered: 24-8-2016
Member Is Offline
Mood: No Mood
|
|
Help with reaction
Recently, when looking for ways to make nitric acid, I found that you could do it by dry distilling CuSO4, KNO3 and KAl(SO4)2. However, there is no
documentation on the formula for this reaction so I was wondering if any of you know.
Kind regards,
Hippo
|
|
hippo
Harmless
Posts: 26
Registered: 24-8-2016
Member Is Offline
Mood: No Mood
|
|
I assume the copper sulphate is as the pentahydrate
|
|
zwt
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 84
Registered: 1-8-2016
Member Is Offline
Mood: No Mood
|
|
The reference in the quote below gives a series of possible reactions.
Quote: Originally posted by entropy51 ![](images/xpblue/lastpost.gif) |
Fifty years ago I had very limited amounts of H2SO4 and I made HNO3 by the dry distillation of KNO3, CuSO4 and alum, but I could not remember the
stoichiometry.
I found a contemporary reference which gives the following quantities: 150 gm of KNO3, 150 gm of CuSO4, and 50 gm of KAl(SO4)2. Yield is said to be
70 gm of about 50% HNO3.
The reference states that the dry distillation was conducted at 800 C, but I believe it must be possible at lower temperatures because I used a Pyrex
retort and it was not damaged. I still have the retort.
This worked fifty years ago and I suspect it will work in the 21st century. I cannot recall my yields, but they were not trivial.
The reference is here: http://www.chemicke-listy.cz/docs/full/2002_12_05.pdf |
|
|