Loading [MathJax]/jax/output/HTML-CSS/fonts/TeX/fontdata.js
Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: This stuff is eating my lab
BlackDragon2712
Hazard to Others
***




Posts: 124
Registered: 22-12-2012
Location: Everywhere
Member Is Offline

Mood: Sleepy

[*] posted on 26-7-2016 at 19:55
This stuff is eating my lab


So I've just came back to my house for vacations and when I check my lab I found this...



20160726_210801.jpg - 4.8MB


It did something to the walls as well... it has like a yellowish powder sticked on it



20160726_210750.jpg - 3.3MB



It is also on my gloves...




20160726_210815.jpg - 3MB



I have no idea of what this could be but here is a list of the stuff I have stored in there:

Mercury metal
Benzoic acid
Sodium acetate
Ammonia
Eugenol
Butanone
Zinc powder
Potassium ferrocyanide
Agar
Dyes
Borax
Potassium permanganate
Phenophthalein
Table salt

Everything is in a separate bottle wrapped in shrink wrap inside a ziploc bag (I did this because my college is in another town so I had to leave my lab secure enough until I come back for vacations)
I honestly don't know what could be causing this, at first I thought it could be the mercury or the ammonia but I am not sure at all... everything is cover with this... gray dust and the walls have this yellow stuff... tomorrow I will clean my lab but I want to get rid of the compound that may be causing this, in the worst case I will get rid of everything I think may be suspicious but I would love to avoid throwing half of my lab away :)

Thanks guys in advance!
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4662
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Preparing to defend myself (academically)

[*] posted on 26-7-2016 at 20:00


It looks like the corrosion caused by hydrochloric acid. I know you don't have it listed there, but that's the only thing that I've seen cause that kind of damage before.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 27-7-2016 at 05:19


Anything that can:
-produce HCl, HBr or HI or the acid itself (acid halides (mineral or organic), haloamines, haloamides, aqua regia (chloride or bromide + HNO3).
-produce Cl2, Br2 or I2 or the halogen itself even in solution into a solvent.
-produce Hg (Mercury is quite volatile and forms amalgams with metals thus protective Zn layer (galvanisation) is chewed and naked iron is exposed to air or to the vapour of your chems.

The two first are the best suspects! Since I have experienced this a lot of time with those.
The corrosion may occur even if the source has dissapeared...so maybe you don't have the bottle of HCl or you I2 drum in there anymore ... the exposure may have been long enough to start the rusting decay...




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
DJF90
International Hazard
*****




Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline

Mood: No Mood

[*] posted on 27-7-2016 at 05:28


It could also be vapours coming from the fridge below the cabinet (assuming you store chems in there...)
View user's profile View All Posts By User
BlackDragon2712
Hazard to Others
***




Posts: 124
Registered: 22-12-2012
Location: Everywhere
Member Is Offline

Mood: Sleepy

[*] posted on 27-7-2016 at 08:38


mmm... Yes I also have chems in that fridge...
Dicloromethane, toluene, chloroform, THF, and a few experiments I couldn't finish.

I had a bottle of 1 L of 32% HCl stored in a different cabinet but it is in a different location (close though) but a third cabinet that is right above the one I used to stored that HCl did not suffered corrosion at all...

I used to store iodine metal in that cabinet but before leaving my house I got rid of it and back then that cabinet was not showing any rust (like 1 year ago)

In the worst case scenario... thinking that it may be the mercury vapors... how can I test for mercury in the air? and how should I proceed with the clean up if it were mercury? I remember reading somewhere that sulfur is used for mercury spills
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 27-7-2016 at 14:09


UV light in front of a white paper display shadow fumes if Hg vapour is present.

HCl 3 cabinets away and I2 from last year in the same cabinet may be responsible...corrosion sometimes is inhibited for unknown reason, but once rusting starts...it goes very fast.




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
diddi
National Hazard
****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 27-7-2016 at 16:36


an interesting idea to check for HCl vapour in the area is to put a small amount of NH3 sln in a beaker nearby. if there is HCl around it will deposit white powder everywhere



Beginning construction of periodic table display
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8071
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 29-7-2016 at 09:54


I also think that this corrosion is from HCl, HBr or free halogen. I do not belive at all that this strong corrosion can be caused by mercury vapor, escaping from a closed container.

I had similar problems, not from HCl itself, but from storage of PCl5, POCl3, PCl3 and SOCl2. All of these are ampouled now and I have no corrosion issues anymore.
I store my HCl in special Schott Duran bottles with GL45 caps having a teflon coated soft silicone liner. I also diluted my 36% HCl to 30%, which strongly reduces the fuming. The 36% acid even caused trouble when stored in the special Schott Duran bottles, but the 30% acid now is stored for years already without any issues.
I also have 48% HBr, also stored in a Schott Duran bottle with GL45 cap. No issues at all.

The corrosion in my lab was really severe. In just a few weeks, all copper materials were covered by a thin green layer and making good electrical contacts was bad. I also stored electronic components and some of these have severely corroded legs, which cannot be soldered anymore. After I discovered that, I have rigorously removed all possible sources of corrosion.

I also store a few bottles of mercury in my lab, but none of them produces any corrosion issues, not even after years of storage.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6367
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 29-7-2016 at 15:48


Off topic...

woelen, I would love to see photos of your lab. I don't think you have ever posted in the Tour my lab thread.

[/off topic]




View user's profile View All Posts By User
BlackDragon2712
Hazard to Others
***




Posts: 124
Registered: 22-12-2012
Location: Everywhere
Member Is Offline

Mood: Sleepy

[*] posted on 29-7-2016 at 18:03


So, at the end it seems that the Iodine metal was the problem... checking a few photos I took the last year I found that the corrosion began the last year and it advanced even when I removed the iodine from that cabinet (the black bottle on the top is the iodine... it is very very annoying since it escapes everything and stains everything)

I also did what PHILOU Zrealone said but I couldn't detect any mercury vapor so those are good news...

Thanks everyone for the help... I'll be more careful with these stuff

Attachment: phpwVd3Mq (3.9MB)
This file has been downloaded 631 times
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8071
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 1-8-2016 at 05:29


One way to store iodine (and also chemicals, producing HCl vapors), is to keep the bottle in a small bucket or jar, in which some NaOH is put in a little dish as well. This exterior bottle must be sealed well, and of course the iodine-bottle must also be sealed. Any iodine vapor, escaping the iodine-bottle, is absorbed by the NaOH. Once every month or so, you need to replace the NaOH by fresh pellets. A small dish with 5 cm diameter and a few mm high, filled with 2 to 3 mm of NaOH-pellets/granules is enough. This method is 100% effective. I use this for storing my small remaining containers of PCl5, POCl3, SOCl2, CH3COCl. The rest (my main stock) of these chemicals is ampouled in glass.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 1-8-2016 at 10:07


I think i mentioned this somewhere before recently. I got 5ltr of 36.2% HCl from APCpure in the UK.

The container has an excellent lid on, i have no idea what its made from but has a gasket on it. I must try and take some pics later, normally the acids are kept in a coldish place (this time of year around 10c).

I forgot a week or so ago while doing the sea shells in HCl, and i left the HCl bottle in a cupboard in my lab, it got to around 22C and when i remembered and went to get the container the sides had swelled a bit.

There was zero sign of escape of the acid though. Not sure if i would use the company again as they messed me about, but i will be keeping the container and reusing it!