Manganese oxide brilliant blue
Old news but colorful
"OSU chemist Mas Subramanian and his team were experimenting with new materials that could be used in electronics applications and they mixed
manganese oxide – which is black in color – with other chemicals and heated them in a furnace to nearly 2,000 degrees Fahrenheit. One of their
samples turned out to be a vivid blue. Oregon State graduate student Andrew Smith initially made these samples to study their electrical properties."
http://oregonstate.edu/ua/ncs/archives/2015/may/licensing-ag...
https://news.artnet.com/art-world/yinmn-blue-to-be-sold-comm...
http://www.dailymail.co.uk/sciencetech/article-3665985/A-dee...
|
|
hyfalcon
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1003
Registered: 29-3-2012
Member Is Offline
Mood: No Mood
|
|
I would be interested in the patent they filed on that one. We've got manganese staining in the hills around my valley that is absolutely black.
Bake some samples in my heat treating furnace see if I turn them blue.
|
|
BromicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
I love the name they are marketing/discussing it under, YInMn blue, a name that certainly appeals to the chemists out there. I am looking forward to
getting some of this pigment (which is already commercially available) and doing some painting with it,
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6252
Registered: 4-10-2014
Location: Unmoved
Member Is Online
Mood: Organised
|
|
YInMn
Does that mean it contains yttrium and indium?
edit
yes.
[Edited on 30-6-2016 by j_sum1]
|
|
crystal grower
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline
Mood: Puzzled
|
|
I have interpreted it in this way too, but Im not sure.
(If yes, It could teoretically be a good source of Y, In for an element collection ).
[Edited on 30-6-2016 by crystal grower]
|
|
PHILOU Zrealone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline
Mood: Bis-diazo-dinitro-hydroquinonic
|
|
Quote: Originally posted by crystal grower ![](images/xpblue/lastpost.gif) |
I have interpreted it in this way too, but Im not sure.
(If yes, It could teoretically be a good source of Y, In for an element collection ).
|
No need to interprete...as explained into the links provided by the OP...it is indeed a mix of Y, In and Mn oxydes...
PH Z (PHILOU Zrealone)
"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1476
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
I looked fruitlessly for 45 min or so last night, trying to find a patent or scientific article on its manufacturing process. Kinda bummed, blue is
my favoritd color. As a matter of fact I bought blue spray enamel yesterday to mark all my tools so they dont walk of the job site.
Kinda figured with the novel electronic properties and crystal structure, there would be resources available. Maybe I should widen my search
parameters, including those terms.. duhh. Regardless, i find it interesting.
|
|
Morgan
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1674
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
A few other tidbits maybe of interest.
"Subramanian has added zinc and titanium to produce a range of purples. He and his team have substituted iron for manganese to produce a new orange
pigment, and they are exploring the use of copper and titanium to make green. Other elements produce yellows and browns."
“We are making new pigments based on a mineral called hibonite, which is normally found in meteorites,” Subramanian says. “They are blue
sometimes, and we are now producing them in our laboratory furnace using cheap raw materials.”
http://oregonstate.edu/terra/2014/10/accidentally-blue/
|
|
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
Here is some better detail about the compound, yttrium indium oxide can hardly be described as cheap I guess that's bull for investors.
www.rsc.org/chemistryworld/2012/09/yr-pigment-paint-chemistr...
From the above link: "So the identification of a new inorganic blue pigment in 2009 looked very promising. Mas Subramanian and coworkers at Oregon
State University, US, found that manganese ions produce an intense blue colour, with the prized ‘reddish’ shade of ultramarine, when they occupy a
trigonal bipyramidal site in metal oxides. The researchers substituted Mn3+ for some indium ions in yttrium indium oxide, forming a solid solution of
YInO3 and YMnO3, which has a blue colour even though the two oxides themselves are white and black, respectively. The depth of the colour varies from
pale blue to virtually black as the manganese content is increased. Inserting manganese into other metal oxides with the same coordination geometry
also offers strong blues. Meanwhile, similar substitutions of iron(iii) and copper(ii) generate bright orange and green pigments. Those are
traditionally less problematic, however, and while the materials may prove to have useful magnetic properties, it’s the blue that has attracted
colour manufacturers."
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1476
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
Hey thanks for that guys. Got some new info and hints for future free time searches
|
|