Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Calcium Sulfate as a desiccant - Will anhydrous work?
RogueRose
International Hazard
*****




Posts: 1590
Registered: 16-6-2014
Member Is Offline


[*] posted on 21-6-2016 at 11:33
Calcium Sulfate as a desiccant - Will anhydrous work?


Wiki states that Anhydrous CaSO4 is very slow to react with water, almost to the point of not absorbing or mixing. It does state there is another form of anhydrous, γ-Anhydrite .05H2O, which will react with water and is mentioned as a commercial desiccant.

The difference in temp between the two anhydrites is 180C and 250C as stated by Wiki. I've found a lot of compounds are very slow to decompose at their stated temp and was wondering if anyone has ever used the pure anhydrous as a desiccant.

View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3621
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 21-6-2016 at 15:29


rock-growing in RBFs seems to be not a popular pastime :D
View user's profile View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 21-6-2016 at 15:45


AFAIK Calcium sulphate is also known as plaster of paris
View user's profile View All Posts By User
Scalebar
Hazard to Self
**




Posts: 54
Registered: 6-5-2016
Location: Europe!
Member Is Offline

Mood: Looking for a way out

[*] posted on 21-6-2016 at 23:37


We used to use it to remove the water during meat analysis - the pulped sample would be mixed with Pet. Ether and a good dollop of anhydrous calcium sulphate and shaken. The ether was then analysed for fat content. This was thirty years ago though...
View user's profile Visit user's homepage View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 22-6-2016 at 01:50


Quote: Originally posted by Scalebar  
We used to use it to remove the water during meat analysis - the pulped sample would be mixed with Pet. Ether and a good dollop of anhydrous calcium sulphate and shaken. The ether was then analysed for fat content. This was thirty years ago though...


IDKW, but that has just put me off Kebabs!
View user's profile View All Posts By User

  Go To Top